EN GJL 200 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.3C/2.4Si/0.7Mn/0.08P/<0.15S

EN GJL 200 Chemical Composition%
CarbonC3.3
IronFe93.4 – 93.5
ManganeseMn0.7
PhosphorusP0.08
SulfurS0 – 0.15
SiliconSi2.4
EN GJL 200 Chemical Composition
Material Standards with Similar Chemical Composition
NBN 83001 FGG20 (Belgium)
GB 9439(88) HT 200 (China)
DS 11301 GG20 (Denmark)
AFNOR NFA32101 FGL200 (France)
DIN 1691 GG15 (Germany)
IS 210 FG200 (India)
UNI 5007 G20 (Italy)
JIS G5501(95) FC200 (Japan)
NEN 6002A GG20 (Netherlands)
NS 722 SjG20 (Norway)
NS 722 SjG250 (Norway)
GOST 1412 SCh20 (Russian Federation)
SABS 1034 200 (South Africa)
ISO 185(88) 200 (International)
BS 1452 200 (United Kingdom)
ASME SA278 30 (USA)
ASTM A126(95) B (USA)
ASTM A278(93) 30 (USA)
ASTM A278M(93) 200 (USA)
ASTM A48(94) 30A (USA)
ASTM A48(94) 30B (USA)
ASTM A48(94) 30C (USA)
ASTM A48(94) 30S (USA)
EN GJL 200 Chemical Composition
EN GJL 200 Chemical Composition

EN GJL 150 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 150 Chemical Composition:

Base Fe (Iron) : Fe/3.2C/2.6Si/0.6Mn/0.1P/<0.15S

ElementMin (%)Max (%)
C (Carbon)3.23.2
Fe (Iron)93.493.5
Mn (Manganese)0.60.6
P (Phosphorus)0.10.1
S (Sulfur)00.15
Si (Silicon)2.62.6
EN GJL 150 Chemical Composition
Material Standards with Similar Chemical Composition
GB 9439(88) HT 150 (China)
AFNOR NFA32101 FGL200A (France)
AFNOR NFA32101 FGL250A (France)
DIN WNr 0.6015 (Germany)
DIN 1691 GG15 (Germany)
UNI 5007 G15 (Italy)
NS 722 SjG200 (Norway)
AS 1830(86) T180 (NSW Australia)
GOST 1412 SCh18 (Russian Federation)
SS 140115 115 (Sweden)
BS 1452 180 (United Kingdom)
ASME SA278 25 (USA)
ASTM A278(93) 25 (USA)
ASTM A278M(93) 175 (USA)
ASTM A48(94) 25A (USA)
ASTM A48(94) 25B (USA)
ASTM A48(94) 25C (USA)
ASTM A48(94) 25S (USA)
EN GJL 150 Chemical Composition (Cast iron, gray, flake graphite)