Aluminum A356.0 permanent mold cast F Processing Properties

PropertyValue
Metal CastingExcellent
Metal Cold FormingUnsuitable
Metal Hot FormingUnsuitable
Metal Press FormingUnsuitable
Metal Deep DrawingUnsuitable
Machining Speed128 m/min
WeldabilityExcellent
(Preheating is not required, post weld heat treatment is required)
Aluminum A356.0 permanent mold cast F Processing Properties

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey