Aluminum A356.0 permanent mold cast F Thermal Properties:
| Property | Value | Unit |
|---|---|---|
| Melting Point | 560 – 610 | °C |
| Maximum Service Temperature | 150 – 170 | °C |
| Minimum Service Temperature | -273 | °C |
| Thermal Conductivity | 149 – 155 | W/m·°C |
| Specific Heat Capacity | 944 – 982 | J/kg·°C |
| Thermal Expansion Coefficient | 20.7 – 22.4 | µstrain/°C |
| Thermal Shock Resistance | 53.5 – 61.1 | °C |
| Thermal Distortion Resistance | 6.75 – 7.38 | MW/m |
| Latent Heat of Fusion | 384 – 393 | kJ/kg |
| Aluminum A356.0 permanent mold cast F Thermal Properties |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey