Aluminum, A356.0, permanent mold cast, F | Thermal Properties

Aluminum A356.0 permanent mold cast F Thermal Properties: Property Value Unit Melting Point 560 – 610 °C Maximum Service Temperature 150 – 170 °C Minimum Service Temperature -273 °C Thermal Conductivity 149 – 155 W/m·°C Specific Heat Capacity 944 – 982 J/kg·°C Thermal Expansion Coefficient 20.7 – 22.4 µstrain/°C Thermal Shock Resistance 53.5 – 61.1 … Continue reading Aluminum, A356.0, permanent mold cast, F | Thermal Properties