Aluminum, A356.0, permanent mold cast, F | Composition

Aluminum A356.0 permanent mold cast F Composition Summary Property Value Composition Al 91-93 / Si 6.5-7.5 / Mg 0.25-0.45 (impurities: Cu < 0.2, Fe < 0.2, Ti < 0.2, Mn < 0.1, Zn < 0.1, Other < 0.15) Material Family Metal (non-ferrous) Base Material Al (Aluminum) Aluminum A356.0 permanent mold cast F Composition Summary Aluminum … Continue reading Aluminum, A356.0, permanent mold cast, F | Composition