Aluminum, A356.0, permanent mold cast, F | General Information
Aluminum A356.0 permanent mold cast F General Information Designation A356.0 (Aluminum Association) Condition F (As-fabricated) UNS Number A13560 EN Number EN AC-42000 / EN AC-Al Si7Mg Aluminum A356.0 permanent mold cast F General Information Aluminum A356.0 permanent mold cast F Typical Uses Typical Uses Applications High-strength alloy for the automotive industry Space frames, wheels, axle … Continue reading Aluminum, A356.0, permanent mold cast, F | General Information