Aluminum, A356.0, permanent mold cast, F | Mechanical Properties

Aluminum A356.0 permanent mold cast F Mechanical Properties Property Value Unit Young’s Modulus 71.5 – 74.5 GPa Specific Stiffness 26.6 – 27.8 MN·m/kg Yield Strength (Elastic Limit) 85.5 – 94.5 MPa Tensile Strength 170 – 187 MPa Specific Strength 31.9 – 35.3 kN·m/kg Elongation 2.5 – 3 % strain Compressive Strength 85.5 – 94.5 MPa … Continue reading Aluminum, A356.0, permanent mold cast, F | Mechanical Properties