PA46 (Polyamide 46 / Nylon 46)

PA46 (Polyamide 46 / Nylon 46)

PA46 Strengths

PA46 (nylon 46) has high impact strength, and it keeps a higher heat distortion temperature and more stiffness at elevated temperature than PA6 or PA66. Its higher crystallinity improves chemical resistance, and although it absorbs about as much water as PA6, it is dimensionally more stable.

PA46 Limitations

It must be processed at high temperature within a narrow window, and its impact properties depend on that processing temperature. Moisture absorption is similar to PA6, and it costs more than PA6 and PA66.

PA46 Designation

PA46, also written 4.6 or 4/6.

PA46 Compositional Summary

(NH(CH2)4NH-CO-(CH2)4-CO)n
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPA46 (Polyamide / nylon 46)
CAS number50327-22-5

PA46 Parts from Turkey

Looking for PA46 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA46 parts in-house and inspects them before shipment.

PA46 Grades

PA46 Unfilled Grades

PA46 Extrusion Grade Material Data Sheet

PA46 General Purpose Grade Material Data Sheet

PA46 Super-Tough Grade Material Data Sheet

PA46 Glass Filled Grades

PA46 15% Glass Fiber Material Data Sheet

PA46 15% Glass Fiber Flame Retarded Material Data Sheet

PA46 30% Glass Fiber Material Data Sheet

PA46 30% Glass Fiber Flame Retarded Material Data Sheet

PA46 50% Glass Fiber Material Data Sheet

PA46 Glass and Mineral Filled Grades

PA46 50% Glass and Mineral Filled Material Data Sheet