PA46 15% Glass Fiber Flame Retarded Material Data Sheet

PA46 15% Glass Fiber Flame Retarded (Polyamide 46) Material Data Sheet

PA46 15% Glass Fiber Flame Retarded Overview

PA46 15% glass fiber flame retarded is a grade of polyamide 46 (PA46, nylon 46), designated Polyamide (Nylon) (Type 46, 15% Glass Fiber, V-0). This PA46 15% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA46 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA46 parts in-house and inspects them before shipment.

PA46 15% Glass Fiber Flame Retarded Designation

Polyamide (Nylon) (Type 46, 15% Glass Fiber, V-0)
TradenamesStanyl

PA46 15% Glass Fiber Flame Retarded Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA46 15% Glass Fiber Flame Retarded Composition detail

Polymer70–80%
Flame retardant5–15%
Glass (fiber)15  %

PA46 15% Glass Fiber Flame Retarded Physical properties

Density1.51–1.54g/cm3

PA46 15% Glass Fiber Flame Retarded Mechanical properties

Young’s modulus4.11–5.13GPa
Specific stiffness2.69–3.37MN.m/kg
Yield strength (elastic limit)61.1–76.3MPa
Tensile strength74.2–90.7MPa
Specific strength40.1–50.1kN.m/kg
Elongation4.6–6.62% strain
Elongation at yield2.71–5.14% strain
Compressive modulus4.39–4.85GPa
Compressive strength94–104MPa
Flexural modulus3.81–4.56GPa
Flexural strength (modulus of rupture)96.3–118MPa
Shear modulus1.64–1.72GPa
Shear strength44.5–54.4MPa
Bulk modulus5.81–6.42GPa
Poisson’s ratio0.36–0.374 
Shape factor6.32
Hardness – Vickers20–22HV
Hardness – Rockwell M131–145 
Hardness – Rockwell R131–145 
Hardness – Shore D86–89 
Elastic stored energy (springs)402–641kJ/m3
Fatigue strength at 10^7 cycles31.3–34.6MPa

PA46 15% Glass Fiber Flame Retarded Impact & fracture properties

Fracture toughness4.17–4.61MPa.m0.5
Toughness (G)3.62–4.84kJ/m2
Impact strength, notched 23 °C6.8–13.2kJ/m2
Impact strength, notched -30 °C3.78–8.22kJ/m2
Impact strength, unnotched 23 °C40.5–59.5kJ/m2
Impact strength, unnotched -30 °C32–48kJ/m2

PA46 15% Glass Fiber Flame Retarded Thermal properties

Melting point284–306°C
Glass temperature71–79°C
Heat deflection temperature 0.45MPa249–302°C
Heat deflection temperature 1.8MPa224–275°C
Maximum service temperature73–87°C
Minimum service temperature-58–-38°C
Thermal conductivity0.41–0.427W/m.°C
Specific heat capacity1330–1380J/kg.°C
Thermal expansion coefficient54.2–55.3µstrain/°C
Thermal shock resistance233–317°C
Thermal distortion resistance0.00747–0.00781MW/m

PA46 15% Glass Fiber Flame Retarded Electrical properties

Electrical resistivity2e14–5e15µohm.cm
Electrical conductivity3.45e-14–8.62e-13%IACS
Dielectric constant (relative permittivity)9.66–13.6 
Dissipation factor (dielectric loss tangent)0.269–0.71 
Dielectric strength (dielectric breakdown)14.8–25.2MV/m
Comparative tracking index200–250V

PA46 15% Glass Fiber Flame Retarded Magnetic properties

Magnetic typeNon-magnetic

PA46 15% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity1640–1840m/s
Mechanical loss coefficient (tan delta)0.0123–0.0136 

PA46 15% Glass Fiber Flame Retarded Absorption & permeability

Water absorption @ 24 hrs1.5–2.5%
Water absorption @ sat6–8%
Humidity absorption @ sat1.6–2.2%

PA46 15% Glass Fiber Flame Retarded Processing properties

Polymer injection moldingAcceptable
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage0.6 – 0.9 %
Melt temperature242 – 316 °C
Mold temperature40 – 80 °C
Molding pressure range34.4 – 103 MPa

PA46 15% Glass Fiber Flame Retarded Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisUnacceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySelf-extinguishing