PA46 50% Glass and Mineral Filled Material Data Sheet

PA46 50% Glass and Mineral Filled (Polyamide 46) Material Data Sheet

PA46 50% Glass and Mineral Filled Overview

PA46 50% glass and mineral filled is a grade of polyamide 46 (PA46, nylon 46), designated Polyamide (Nylon) (Type 46, 50% Glass and Mineral Filled). This PA46 50% glass and mineral filled material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA46 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA46 parts in-house and inspects them before shipment.

PA46 50% Glass and Mineral Filled Designation

Polyamide (Nylon) (Type 46, 50% Glass and Mineral Filled)
TradenamesStanyl

PA46 50% Glass and Mineral Filled Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA46 50% Glass and Mineral Filled Composition detail

Polymer50  %
Glass (fiber)15–35%
Mineral (unspecified)15–35%

PA46 50% Glass and Mineral Filled Physical properties

Density1.63–1.66g/cm3

PA46 50% Glass and Mineral Filled Mechanical properties

Young’s modulus8.29–10.3GPa
Specific stiffness5.04–6.26MN.m/kg
Yield strength (elastic limit)85.8–107MPa
Tensile strength86.7–106MPa
Specific strength52.1–65.1kN.m/kg
Elongation2.49–3.58% strain
Elongation at yield2.1–3.98% strain
Compressive modulus8.85–9.78GPa
Compressive strength110–121MPa
Flexural modulus7.66–9.17GPa
Flexural strength (modulus of rupture)120–147MPa
Shear modulus3.37–3.55GPa
Shear strength52–63.6MPa
Bulk modulus9.64–10.7GPa
Poisson’s ratio0.333–0.347 
Shape factor8.01
Hardness – Vickers28–30HV
Hardness – Rockwell M142–157 
Hardness – Rockwell R142–157 
Hardness – Shore D88–92 
Elastic stored energy (springs)394–626kJ/m3
Fatigue strength at 10^7 cycles36.6–40.5MPa

PA46 50% Glass and Mineral Filled Impact & fracture properties

Fracture toughness4.8–5.31MPa.m0.5
Toughness (G)2.39–3.18kJ/m2
Impact strength, notched 23 °C6.12–11.9kJ/m2
Impact strength, notched -30 °C3.31–7.19kJ/m2
Impact strength, unnotched 23 °C33.4–49.1kJ/m2
Impact strength, unnotched -30 °C30–45kJ/m2

PA46 50% Glass and Mineral Filled Thermal properties

Melting point284–306°C
Glass temperature71–79°C
Heat deflection temperature 0.45MPa284–340°C
Heat deflection temperature 1.8MPa258–313°C
Maximum service temperature73–87°C
Minimum service temperature-58–-38°C
Thermal conductivity0.569–0.592W/m.°C
Specific heat capacity1250–1300J/kg.°C
Thermal expansion coefficient30.2–30.8µstrain/°C
Thermal shock resistance292–396°C
Thermal distortion resistance0.0186–0.0195MW/m

PA46 50% Glass and Mineral Filled Electrical properties

Electrical resistivity2e15–5e16µohm.cm
Electrical conductivity3.45e-15–8.62e-14%IACS
Dielectric constant (relative permittivity)13.3–18.7 
Dissipation factor (dielectric loss tangent)0.33–0.87 
Dielectric strength (dielectric breakdown)14.8–25.2MV/m
Comparative tracking index325–375V

PA46 50% Glass and Mineral Filled Magnetic properties

Magnetic typeNon-magnetic

PA46 50% Glass and Mineral Filled Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2240–2510m/s
Mechanical loss coefficient (tan delta)0.00866–0.00958 

PA46 50% Glass and Mineral Filled Absorption & permeability

Water absorption @ 24 hrs1.4–2.4%
Water absorption @ sat5.8–7.7%
Humidity absorption @ sat1.5–2.1%

PA46 50% Glass and Mineral Filled Processing properties

Polymer injection moldingAcceptable
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage0.3 – 0.6 %
Melt temperature242 – 316 °C
Mold temperature40 – 80 °C
Molding pressure range34.4 – 103 MPa

PA46 50% Glass and Mineral Filled Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisUnacceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning