Home » PA (Polyamide / Nylon) » PA46 (Polyamide 46 / Nylon 46) » PA46 Glass Filled Grades » PA46 30% Glass Fiber Flame Retarded Material Data Sheet
PA46 30% Glass Fiber Flame Retarded (Polyamide 46) Material Data Sheet
PA46 30% Glass Fiber Flame Retarded Overview
PA46 30% glass fiber flame retarded is a grade of polyamide 46 (PA46, nylon 46), designated Polyamide (Nylon) (Type 46, 30% Glass Fiber, V-0). This PA46 30% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA46 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA46 parts in-house and inspects them before shipment.
PA46 30% Glass Fiber Flame Retarded Designation
Polyamide (Nylon) (Type 46, 30% Glass Fiber, V-0) Tradenames Hifill, Stanyl
PA46 30% Glass Fiber Flame Retarded Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA46 30% Glass Fiber Flame Retarded Composition detail
Polymer 55 – 65 % Flame retardant 5 – 15 % Glass (fiber) 30 %
PA46 30% Glass Fiber Flame Retarded Physical properties
PA46 30% Glass Fiber Flame Retarded Mechanical properties
Young’s modulus 7.12 – 8.88 GPa Specific stiffness 4.35 – 5.43 MN.m/kg Yield strength (elastic limit) 111 – 139 MPa Tensile strength 113 – 138 MPa Specific strength 67.9 – 85 kN.m/kg Elongation 2.87 – 4.13 % strain Elongation at yield 2.42 – 4.59 % strain Compressive modulus 7.6 – 8.4 GPa Compressive strength 143 – 158 MPa Flexural modulus 6.53 – 7.82 GPa Flexural strength (modulus of rupture) 165 – 202 MPa Shear modulus 2.87 – 3.01 GPa Shear strength 67.5 – 82.5 MPa Bulk modulus 9.05 – 10 GPa Poisson’s ratio 0.346 – 0.36 Shape factor 6.13 Hardness – Vickers 36 – 39 HV Hardness – Rockwell M 161 – 178 Hardness – Rockwell R 161 – 178 Hardness – Shore D 93 – 97 Elastic stored energy (springs) 767 – 1230 kJ/m3 Fatigue strength at 10^7 cycles 47.5 – 52.5 MPa
PA46 30% Glass Fiber Flame Retarded Impact & fracture properties
Fracture toughness 4.66 – 5.15 MPa.m0.5 Toughness (G) 2.61 – 3.49 kJ/m2 Impact strength, notched 23 °C 7.48 – 14.5 kJ/m2 Impact strength, notched -30 °C 6.3 – 13.7 kJ/m2 Impact strength, unnotched 23 °C 48.6 – 71.4 kJ/m2 Impact strength, unnotched -30 °C 40 – 60 kJ/m2
PA46 30% Glass Fiber Flame Retarded Thermal properties
Melting point 284 – 306 °C Glass temperature 71 – 79 °C Heat deflection temperature 0.45MPa 284 – 340 °C Heat deflection temperature 1.8MPa 258 – 313 °C Maximum service temperature 73 – 87 °C Minimum service temperature -58 – -38 °C Thermal conductivity 0.507 – 0.527 W/m.°C Specific heat capacity 1210 – 1260 J/kg.°C Thermal expansion coefficient 37.4 – 38.2 µstrain/°C Thermal shock resistance 354 – 482 °C Thermal distortion resistance 0.0134 – 0.014 MW/m
PA46 30% Glass Fiber Flame Retarded Electrical properties
Electrical resistivity 1.51e15 – 3.76e16 µohm.cm Electrical conductivity 4.59e-15 – 1.14e-13 %IACS Dielectric constant (relative permittivity) 8.3 – 11.7 Dissipation factor (dielectric loss tangent) 0.182 – 0.479 Dielectric strength (dielectric breakdown) 14.8 – 25.2 MV/m Comparative tracking index 300 – 350 V
PA46 30% Glass Fiber Flame Retarded Magnetic properties
Magnetic type Non-magnetic
PA46 30% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2080 – 2330 m/s Mechanical loss coefficient (tan delta) 0.00938 – 0.0104
PA46 30% Glass Fiber Flame Retarded Absorption & permeability
Water absorption @ 24 hrs 1.2 – 2 % Water absorption @ sat 4.9 – 6.5 % Humidity absorption @ sat 1.4 – 1.9 %
PA46 30% Glass Fiber Flame Retarded Processing properties
Polymer injection molding Acceptable Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 0.4 – 0.6 % Melt temperature 242 – 316 °C Mold temperature 40 – 80 °C Molding pressure range 34.4 – 103 MPa
PA46 30% Glass Fiber Flame Retarded Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Unacceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing