PA46 15% Glass Fiber (Polyamide 46) Material Data Sheet
PA46 15% Glass Fiber Overview
PA46 15% glass fiber is a grade of polyamide 46 (PA46, nylon 46), designated Polyamide (Nylon) (Type 46, 15% Glass Fiber). This PA46 15% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA46 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA46 parts in-house and inspects them before shipment.
PA46 15% Glass Fiber Designation
Polyamide (Nylon) (Type 46, 15% Glass Fiber)
Tradenames
Stanyl, Sup-Tech
PA46 15% Glass Fiber Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA46 15% Glass Fiber Composition detail
Polymer
85
%
Glass (fiber)
15
%
PA46 15% Glass Fiber Physical properties
Density
1.28
–
1.3
g/cm3
PA46 15% Glass Fiber Mechanical properties
Young’s modulus
2.49
–
3.11
GPa
Specific stiffness
1.93
–
2.41
MN.m/kg
Yield strength (elastic limit)
51.9
–
64.8
MPa
Tensile strength
63
–
77
MPa
Specific strength
40.2
–
50.2
kN.m/kg
Elongation
6.56
–
9.44
% strain
Elongation at yield
3.86
–
7.33
% strain
Compressive modulus
2.66
–
2.94
GPa
Compressive strength
79.8
–
88.2
MPa
Flexural modulus
2.31
–
2.77
GPa
Flexural strength (modulus of rupture)
75
–
91.6
MPa
Shear modulus
0.989
–
1.04
GPa
Shear strength
37.8
–
46.2
MPa
Bulk modulus
3.69
–
4.08
GPa
Poisson’s ratio
0.365
–
0.38
Shape factor
5.19
Hardness – Vickers
17
–
18
HV
Hardness – Rockwell M
120
–
133
Hardness – Rockwell R
120
–
133
Hardness – Shore D
83
–
86
Elastic stored energy (springs)
479
–
763
kJ/m3
Fatigue strength at 10^7 cycles
26.6
–
29.4
MPa
PA46 15% Glass Fiber Impact & fracture properties
Fracture toughness
3.77
–
4.16
MPa.m0.5
Toughness (G)
4.88
–
6.51
kJ/m2
Impact strength, notched 23 °C
8.84
–
17.2
kJ/m2
Impact strength, notched -30 °C
3.78
–
8.22
kJ/m2
Impact strength, unnotched 23 °C
81
–
119
kJ/m2
Impact strength, unnotched -30 °C
40
–
60
kJ/m2
PA46 15% Glass Fiber Thermal properties
Melting point
284
–
306
°C
Glass temperature
71
–
79
°C
Heat deflection temperature 0.45MPa
249
–
302
°C
Heat deflection temperature 1.8MPa
224
–
275
°C
Maximum service temperature
73
–
87
°C
Minimum service temperature
-58
–
-38
°C
Thermal conductivity
0.367
–
0.382
W/m.°C
Specific heat capacity
1450
–
1510
J/kg.°C
Thermal expansion coefficient
65.5
–
66.8
µstrain/°C
Thermal shock resistance
270
–
368
°C
Thermal distortion resistance
0.00554
–
0.00579
MW/m
PA46 15% Glass Fiber Electrical properties
Electrical resistivity
2e14
–
5e15
µohm.cm
Electrical conductivity
3.45e-14
–
8.62e-13
%IACS
Dielectric constant (relative permittivity)
14.2
–
20
Dissipation factor (dielectric loss tangent)
0.269
–
0.71
Dielectric strength (dielectric breakdown)
14.8
–
25.2
MV/m
Comparative tracking index
400
–
450
V
PA46 15% Glass Fiber Magnetic properties
Magnetic type
Non-magnetic
PA46 15% Glass Fiber Optical, aesthetic and acoustic properties