Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Glass Filled Grades » PA66 50% Glass Fiber Material Data Sheet
PA66 50% Glass Fiber (Polyamide 66) Material Data Sheet
PA66 50% Glass Fiber Overview
PA66 50% glass fiber is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 50% Glass Fiber). This PA66 50% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 50% Glass Fiber Designation
Polyamide (Nylon) (Type 66, 50% Glass Fiber) Tradenames Akromid, Altech, Aquaforce, Ashlene, Badamid, Bergamid, Celstran, Compamid, Durethan, Edgetek, Latamid, Leona, LNP Thermocomp, Niretan, Nylaforce, Nypol, Pentamid, Plustek, Polybest, Polytron, Radilon, Scanamid, Schulamid, Slovamid, Staramide, Strator, Technyl, Tecomid, Terez, Tislamid, Torzen, Ultramid, Vitamide, Wellamid
PA66 50% Glass Fiber Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA66 50% Glass Fiber Composition detail
Polymer 50 % Glass (fiber) 50 %
PA66 50% Glass Fiber Physical properties
PA66 50% Glass Fiber Mechanical properties
Young’s modulus 10.9 – 13.6 GPa Specific stiffness 6.92 – 8.64 MN.m/kg Yield strength (elastic limit) 156 – 194 MPa Tensile strength 159 – 194 MPa Specific strength 99 – 123 kN.m/kg Elongation 2.62 – 3.78 % strain Elongation at yield 2.21 – 4.19 % strain Compressive modulus 11.6 – 12.8 GPa Compressive strength 201 – 222 MPa Flexural modulus 9.1 – 10.9 GPa Flexural strength (modulus of rupture) 225 – 275 MPa Shear modulus 4.44 – 4.66 GPa Shear strength 95.3 – 117 MPa Bulk modulus 12.3 – 13.6 GPa Poisson’s ratio 0.329 – 0.343 Shape factor 6.5 Hardness – Vickers 50 – 55 HV Hardness – Rockwell M 184 – 204 Hardness – Rockwell R 184 – 204 Hardness – Brinell 117 – 147 HB Hardness – Shore D 98 – 102 Elastic stored energy (springs) 988 – 1560 kJ/m3 Fatigue strength at 10^7 cycles 67.1 – 74.1 MPa
PA66 50% Glass Fiber Impact & fracture properties
Fracture toughness 5.07 – 5.61 MPa.m0.5 Toughness (G) 2.02 – 2.7 kJ/m2 Impact strength, notched 23 °C 17.5 – 34 kJ/m2 Impact strength, notched -30 °C 13.4 – 29.2 kJ/m2 Impact strength, unnotched 23 °C 83.4 – 123 kJ/m2 Impact strength, unnotched -30 °C 75.7 – 113 kJ/m2
PA66 50% Glass Fiber Thermal properties
Melting point 250 – 271 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 225 – 276 °C Heat deflection temperature 1.8MPa 225 – 276 °C Maximum service temperature 90 – 130 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.586 – 0.61 W/m.°C Specific heat capacity 1280 – 1330 J/kg.°C Thermal expansion coefficient 58.3 – 60.7 µstrain/°C Thermal shock resistance 206 – 280 °C Thermal distortion resistance 0.00978 – 0.0103 MW/m
PA66 50% Glass Fiber Electrical properties
Electrical resistivity 2.23e19 – 5.57e20 µohm.cm Electrical conductivity 3.1e-19 – 7.73e-18 %IACS Dielectric constant (relative permittivity) 9.63 – 13.6 Dissipation factor (dielectric loss tangent) 0.101 – 0.265 Dielectric strength (dielectric breakdown) 35.8 – 60.9 MV/m Comparative tracking index 450 – 550 V
PA66 50% Glass Fiber Magnetic properties
Magnetic type Non-magnetic
PA66 50% Glass Fiber Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2630 – 2940 m/s Mechanical loss coefficient (tan delta) 0.00795 – 0.00878
PA66 50% Glass Fiber Absorption & permeability
Water absorption @ 24 hrs 0.46 – 0.74 % Water absorption @ sat 3.8 – 5 % Humidity absorption @ sat 1.1 – 1.4 %
PA66 50% Glass Fiber Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.091 – 0.11 % Melt temperature 235 – 310 °C Mold temperature 40 – 60 °C Molding pressure range 68.8 – 138 MPa
PA66 50% Glass Fiber Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning
Modulus Metal Services
Manufacturing & Quality Services in Turkey