Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Glass Filled Grades » PA66 40% Glass Fiber Lubricated Material Data Sheet
PA66 40% Glass Fiber Lubricated (Polyamide 66) Material Data Sheet
PA66 40% Glass Fiber Lubricated Overview
PA66 40% glass fiber lubricated is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 40% Glass Fiber, Lubricated, 5-20% PTFE). This PA66 40% glass fiber lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 40% Glass Fiber Lubricated Designation
Polyamide (Nylon) (Type 66, 40% Glass Fiber, Lubricated, 5-20% PTFE) Tradenames Eplamid, Latilub, LNP Lubricomp, Luvocom, Nypol, RTP, Tribocomp, Vitamide
PA66 40% Glass Fiber Lubricated Typical uses
Automotive applications, bearings, business equipment, gears, parts (engineering), switches, textile applications
PA66 40% Glass Fiber Lubricated Composition detail
Polymer 40 – 55 % PTFE (lubricant) 5 – 20 % Glass (fiber) 40 %
PA66 40% Glass Fiber Lubricated Physical properties
PA66 40% Glass Fiber Lubricated Mechanical properties
Young’s modulus 10.3 – 13.4 GPa Specific stiffness 6.68 – 8.81 MN.m/kg Yield strength (elastic limit) 139 – 162 MPa Tensile strength 168 – 204 MPa Specific strength 89.3 – 107 kN.m/kg Elongation 2 – 3 % strain Elongation at yield 2 – 4 % strain Compressive modulus 6.88 – 7.23 GPa Compressive strength 124 – 138 MPa Flexural modulus 8.96 – 12.4 GPa Flexural strength (modulus of rupture) 252 – 294 MPa Shear modulus 4.25 – 4.47 GPa Shear strength 103 – 120 MPa Bulk modulus 11.5 – 12 GPa Poisson’s ratio 0.34 – 0.354 Shape factor 7 Hardness – Vickers 42 – 46 HV Hardness – Rockwell R 120 – 122 Hardness – Shore D 92 – 102 Elastic stored energy (springs) 785 – 1160 kJ/m3 Fatigue strength at 10^7 cycles 50.9 – 59.4 MPa
PA66 40% Glass Fiber Lubricated Impact & fracture properties
Fracture toughness 7.21 – 8.73 MPa.m0.5 Toughness (G) 4.31 – 6.67 kJ/m2 Impact strength, notched 23 °C 11.6 – 15.8 kJ/m2 Impact strength, notched -30 °C 11.1 – 13.4 kJ/m2 Impact strength, unnotched 23 °C 50.6 – 126 kJ/m2 Impact strength, unnotched -30 °C 50 kJ/m2
PA66 40% Glass Fiber Lubricated Thermal properties
Melting point 250 – 265 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 245 – 270 °C Heat deflection temperature 1.8MPa 240 – 260 °C Vicat softening point 250 °C Maximum service temperature 107 – 127 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.52 W/m.°C Specific heat capacity 1480 – 1530 J/kg.°C Thermal expansion coefficient 24 – 36 µstrain/°C Thermal shock resistance 339 – 553 °C Thermal distortion resistance 0.0144 – 0.0217 MW/m
PA66 40% Glass Fiber Lubricated Electrical properties
Electrical resistivity 1e20 – 1e22 µohm.cm Electrical conductivity 1.72e-20 – 1.72e-18 %IACS Dielectric constant (relative permittivity) 3.8 Dissipation factor (dielectric loss tangent) 0.015 Dielectric strength (dielectric breakdown) 20 – 37 MV/m Comparative tracking index 450 – 500 V
PA66 40% Glass Fiber Lubricated Magnetic properties
Magnetic type Non-magnetic
PA66 40% Glass Fiber Lubricated Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2580 – 2980 m/s Mechanical loss coefficient (tan delta) 0.00671 – 0.00888
PA66 40% Glass Fiber Lubricated Absorption & permeability
Water absorption @ 24 hrs 0.5 – 1 % Water absorption @ sat 4.1 % Humidity absorption @ sat 0.86 – 1.2 %
PA66 40% Glass Fiber Lubricated Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.2 – 0.4 % Melt temperature 260 – 304 °C Mold temperature 65.6 – 120 °C Molding pressure range 68.9 – 138 MPa
PA66 40% Glass Fiber Lubricated Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning