PA66 30% Long Glass Fiber Overview

PA66 30% long glass fiber is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 30% Long Glass Fiber). This PA66 30% long glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 30% Long Glass Fiber Designation

Polyamide (Nylon) (Type 66, 30% Long Glass Fiber)
TradenamesAshlene, Celstran, Complet, Polytron

PA66 30% Long Glass Fiber Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 30% Long Glass Fiber Composition detail

Polymer70  %
Glass (fiber)30  %

PA66 30% Long Glass Fiber Physical properties

Density1.36–1.39g/cm3

PA66 30% Long Glass Fiber Mechanical properties

Young’s modulus5.9–7.36GPa
Specific stiffness4.29–5.36MN.m/kg
Yield strength (elastic limit)112–139MPa
Tensile strength113–138MPa
Specific strength81.4–101kN.m/kg
Elongation3.03–4.36% strain
Elongation at yield2.55–4.84% strain
Compressive modulus6.3–6.96GPa
Compressive strength143–158MPa
Flexural modulus5.95–7.13GPa
Flexural strength (modulus of rupture)164–201MPa
Shear modulus2.38–2.5GPa
Shear strength67.7–82.8MPa
Bulk modulus7.5–8.29GPa
Poisson’s ratio0.34–0.36 
Shape factor5.47
Hardness – Vickers36–40HV
Hardness – Rockwell M162–179 
Hardness – Rockwell R162–179 
Hardness – Shore D93–97 
Elastic stored energy (springs)940–1480kJ/m3
Fatigue strength at 10^7 cycles47.7–52.7MPa

PA66 30% Long Glass Fiber Impact & fracture properties

Fracture toughness4.48–4.95MPa.m0.5
Toughness (G)2.91–3.89kJ/m2
Impact strength, notched 23 °C15.2–29.5kJ/m2
Impact strength, notched -30 °C10.8–23.5kJ/m2
Impact strength, unnotched 23 °C68.7–101kJ/m2

PA66 30% Long Glass Fiber Thermal properties

Melting point260–265°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa237–290°C
Heat deflection temperature 1.8MPa252–257°C
Maximum service temperature90–130°C
Minimum service temperature-81–-71°C
Thermal conductivity0.436–0.453W/m.°C
Specific heat capacity1350–1450J/kg.°C
Thermal expansion coefficient41.2–43µstrain/°C
Thermal shock resistance386–524°C
Thermal distortion resistance0.0102–0.0109MW/m

PA66 30% Long Glass Fiber Electrical properties

Electrical resistivity2e17–5e18µohm.cm
Electrical conductivity3.45e-17–8.62e-16%IACS
Dielectric constant (relative permittivity)8.56–12.1 
Dissipation factor (dielectric loss tangent)0.136–0.358 
Dielectric strength (dielectric breakdown)27.8–47.3MV/m
Comparative tracking index475–525V

PA66 30% Long Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PA66 30% Long Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2070–2320m/s
Mechanical loss coefficient (tan delta)0.00983–0.0109 

PA66 30% Long Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.51–0.83%
Water absorption @ sat5–6.6%
Humidity absorption @ sat1.4–1.9%

PA66 30% Long Glass Fiber Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.273 – 0.33 %
Melt temperature223 – 299 °C
Mold temperature40 – 60 °C
Molding pressure range68.8 – 138 MPa

PA66 30% Long Glass Fiber Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning