Home » PA (Polyamide / Nylon) » PA6 (Polyamide 6 / Nylon 6) » PA6 Glass Filled Grades » PA6 33% Glass Fiber Toughened Material Data Sheet
PA6 33% Glass Fiber Toughened (Polyamide 6) Material Data Sheet
PA6 33% Glass Fiber Toughened Overview
PA6 33% glass fiber toughened is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, 33% Glass Fiber, Toughened). This PA6 33% glass fiber toughened material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.
PA6 33% Glass Fiber Toughened Designation
Polyamide (Nylon) (Type 6, 33% Glass Fiber, Toughened) Tradenames Adell, Chemlon, Durethan, Ultramid
PA6 33% Glass Fiber Toughened Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA6 33% Glass Fiber Toughened Composition detail
Polymer 52 – 64 % Impact modifier 3 – 15 % Glass (fiber) 33 %
PA6 33% Glass Fiber Toughened Physical properties
PA6 33% Glass Fiber Toughened Mechanical properties
Young’s modulus 6.34 – 7.91 GPa Specific stiffness 4.64 – 5.8 MN.m/kg Yield strength (elastic limit) 103 – 129 MPa Tensile strength 104 – 128 MPa Specific strength 75.4 – 94.6 kN.m/kg Elongation 5.33 – 7.67 % strain Elongation at yield 4.49 – 8.52 % strain Compressive modulus 6.77 – 7.48 GPa Compressive strength 132 – 146 MPa Flexural modulus 5.01 – 6 GPa Flexural strength (modulus of rupture) 117 – 143 MPa Shear modulus 2.55 – 2.68 GPa Shear strength 62.6 – 76.6 MPa Bulk modulus 8.06 – 8.91 GPa Poisson’s ratio 0.34 – 0.36 Shape factor 5.97 Hardness – Vickers 33 – 37 HV Hardness – Rockwell M 156 – 172 Hardness – Rockwell R 156 – 172 Hardness – Shore D 92 – 95 Elastic stored energy (springs) 741 – 1190 kJ/m3 Fatigue strength at 10^7 cycles 44.1 – 48.7 MPa
PA6 33% Glass Fiber Toughened Impact & fracture properties
Fracture toughness 4.55 – 5.03 MPa.m0.5 Toughness (G) 2.8 – 3.74 kJ/m2 Impact strength, notched 23 °C 15.6 – 30.4 kJ/m2 Impact strength, notched -30 °C 9.61 – 20.9 kJ/m2 Impact strength, unnotched 23 °C 74.5 – 109 kJ/m2 Impact strength, unnotched -30 °C 68 – 102 kJ/m2
PA6 33% Glass Fiber Toughened Thermal properties
Melting point 210 – 220 °C Glass temperature 44 – 56 °C Heat deflection temperature 0.45MPa 198 – 246 °C Heat deflection temperature 1.8MPa 182 – 228 °C Maximum service temperature 57 – 77 °C Minimum service temperature -64 – -54 °C Thermal conductivity 0.41 – 0.427 W/m.°C Specific heat capacity 1430 – 1490 J/kg.°C Thermal expansion coefficient 54.2 – 55.3 µstrain/°C Thermal shock resistance 255 – 347 °C Thermal distortion resistance 0.00748 – 0.00782 MW/m
PA6 33% Glass Fiber Toughened Electrical properties
Electrical resistivity 2e17 – 5e18 µohm.cm Electrical conductivity 3.45e-17 – 8.62e-16 %IACS Dielectric constant (relative permittivity) 10 – 14.2 Dissipation factor (dielectric loss tangent) 0.033 – 0.087 Dielectric strength (dielectric breakdown) 21.5 – 36.5 MV/m Comparative tracking index 475 V
PA6 33% Glass Fiber Toughened Magnetic properties
Magnetic type Non-magnetic
PA6 33% Glass Fiber Toughened Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2150 – 2410 m/s Mechanical loss coefficient (tan delta) 0.0107 – 0.0118
PA6 33% Glass Fiber Toughened Absorption & permeability
Water absorption @ 24 hrs 0.98 – 1.6 % Water absorption @ sat 4.3 – 5.7 % Humidity absorption @ sat 1 – 1.4 %
PA6 33% Glass Fiber Toughened Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.1 – 0.3 % Melt temperature 215 – 288 °C Mold temperature 50 – 60 °C Molding pressure range 68.8 – 138 MPa
PA6 33% Glass Fiber Toughened Durability
Water (fresh) Excellent Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Limited use Strong alkalis Limited use Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning