PA6 30% Long Glass Fiber Material Data Sheet

PA6 30% Long Glass Fiber (Polyamide 6) Material Data Sheet

PA6 30% Long Glass Fiber Overview

PA6 30% long glass fiber is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, 30% Long Glass Fiber). This PA6 30% long glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.

PA6 30% Long Glass Fiber Designation

Polyamide (Nylon) (Type 6, 30% Long Glass Fiber)
TradenamesCelstran, Complet, Sepaz, Stranox

PA6 30% Long Glass Fiber Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA6 30% Long Glass Fiber Composition detail

Polymer70  %
Glass (fiber)30  %

PA6 30% Long Glass Fiber Physical properties

Density1.34–1.37g/cm3

PA6 30% Long Glass Fiber Mechanical properties

Young’s modulus6.5–8.1GPa
Specific stiffness4.8–5.98MN.m/kg
Yield strength (elastic limit)111–139MPa
Tensile strength113–138MPa
Specific strength81.9–103kN.m/kg
Elongation2.81–4.05% strain
Elongation at yield2.37–4.5% strain
Compressive modulus6.94–7.67GPa
Compressive strength143–158MPa
Flexural modulus5.82–6.98GPa
Flexural strength (modulus of rupture)176–215MPa
Shear modulus2.62–2.75GPa
Shear strength67.5–82.5MPa
Bulk modulus8.26–9.13GPa
Poisson’s ratio0.34–0.36 
Shape factor5.8
Hardness – Vickers36–39HV
Hardness – Rockwell M161–178 
Hardness – Rockwell R161–178 
Hardness – Shore D93–97 
Elastic stored energy (springs)840–1340kJ/m3
Fatigue strength at 10^7 cycles47.5–52.5MPa

PA6 30% Long Glass Fiber Impact & fracture properties

Fracture toughness4.57–5.05MPa.m0.5
Toughness (G)2.75–3.67kJ/m2
Impact strength, notched 23 °C23.8–46.2kJ/m2
Impact strength, notched -30 °C6.72–14.6kJ/m2
Impact strength, unnotched 23 °C46.8–68.8kJ/m2
Impact strength, unnotched -30 °C37.3–56kJ/m2

PA6 30% Long Glass Fiber Thermal properties

Melting point210–220°C
Glass temperature44–56°C
Heat deflection temperature 0.45MPa195–220°C
Heat deflection temperature 1.8MPa192–240°C
Maximum service temperature90–130°C
Minimum service temperature-64–-54°C
Thermal conductivity0.445–0.463W/m.°C
Specific heat capacity1350–1450J/kg.°C
Thermal expansion coefficient38.9–40.3µstrain/°C
Thermal shock resistance370–505°C
Thermal distortion resistance0.0112–0.0118MW/m

PA6 30% Long Glass Fiber Electrical properties

Electrical resistivity2.53e19–6.32e20µohm.cm
Electrical conductivity2.73e-19–6.81e-18%IACS
Dielectric constant (relative permittivity)10.1–14.2 
Dissipation factor (dielectric loss tangent)0.117–0.309 
Dielectric strength (dielectric breakdown)25.1–42.7MV/m
Comparative tracking index500–550V

PA6 30% Long Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PA6 30% Long Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2190–2450m/s
Mechanical loss coefficient (tan delta)0.00994–0.011 

PA6 30% Long Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.72–1.2%
Water absorption @ sat5.4–7.2%
Humidity absorption @ sat1.7–2.3%

PA6 30% Long Glass Fiber Processing properties

Polymer injection moldingAcceptable
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.3 – 0.9 %
Melt temperature198 – 288 °C
Mold temperature50 – 60 °C
Molding pressure range68.8 – 138 MPa

PA6 30% Long Glass Fiber Durability

Water (fresh)Excellent
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisLimited use
Strong alkalisLimited use
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning