Custom 450 H1050 Stainless Steel Material Data Sheet
Custom 450 H1050 Stainless Steel Material Data Sheet (Martensitic, Precipitation Hardened)
Custom 450 H1050 Stainless Steel Overview
Custom 450 H1050 stainless steel is a martensitic precipitation hardening stainless steel (UNS S45000) in the wrought form. Condition: H1050 (Solution annealed; precipitation (age) hardened at 566°C; air cooled). This Custom 450 H1050 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for Custom 450 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined Custom 450 parts in-house and inspects them before shipment.
Custom 450 Designation
Custom 450, wrought
Condition
H1050 (Solution annealed; precipitation (age) hardened at 566°C; air cooled)
UNS number
S45000
US name
Custom 450
Custom 450 Typical uses
Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes