Base Fe (Iron) : Fe/3.1C/2.1Si/0.55Mn/trace P, S
| Element | % | |
|---|---|---|
| C (Carbon) | 3.1 | |
| Fe (Iron) | 94.3 | |
| Mn (Manganese) | 0.55 | |
| P (Phosphorus) | 1e-9 | |
| S (Sulfur) | 1e-9 | |
| Si (Silicon) | 2.1 | |
| EN GJL 250 Chemical Composition |
| Material Standards with Similar Chemical Composition |
|---|
| ASTM A126(95) C (USA) |
| ASTM A48(94) 40A (USA) |
| ASTM A48(94) 40B (USA) |
| ASTM A48(94) 40C (USA) |
| ASTM A48(94) 40S (USA) |