PEK (Polyetherketone)

PEK (Polyetherketone)

PEK Overview

PEK (polyetherketone) is a high-temperature semi-crystalline thermoplastic of the polyether ketone family.

PEK Strengths

PEK has higher melting and glass transition temperatures than PEEK, though lower than PEKK, and slightly better stiffness and tensile strength than PEEK.

PEK Limitations

It costs more than PEEK and needs even higher mold temperatures than PEEK, which are already high.

PEK Designation

Chemical name: poly(oxy-1,4-phenylenecarbonyl-1,4-phenylene). Tradenames include Ultrapek, Luvocom and PEEK-HT.

Typical Uses of PEK

Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, tire pressure sensor housings, valve spring discs, rollers, guides, gears and reciprocating components.

PEK Compositional Summary

(-C6H4-O-C6H4-(C=O)-)n
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPEK (Polyetherketone)
CAS number27380-27-4

Effect of Composition on PEK

A higher share of ketone groups (33% in PEEK, 50% in PEK, 67% in PEKK) raises the melting and glass transition temperatures. Other properties change little, apart from a small gain in stiffness and tensile strength.

PEK Processing Properties

First Commercial Production

1986

Forming

PEK can be compression molded, injection molded, extruded and vacuum formed. It needs very high melt temperatures, and pre-drying is essential because of the high mold temperatures. Fine powder can coat metal parts up to about 2 mm thick by vortex sintering.

Machining

The material machines very easily. Carbide or diamond-tipped tools with water cooling are recommended, and the parts should be annealed before machining.

Joining

Solvent bonding is difficult, but a wide range of adhesives works well, and surface treatment such as laser treatment greatly improves bond strength. All welding methods except radio-frequency welding are suitable, although hot gas welding is difficult and the high melting point means welding needs a lot of energy. Laser welding works, the material can be welded to PEI, and welds to aluminum have had some success. Films can be heat sealed at high temperatures.

Surface Treatment

PEK can be painted.

PEK Grades

Unfilled PEK

PEK (unfilled)

Glass Filled PEK

PEK (20% glass fiber)

PEK (30% glass fiber)

PEK (40% glass fiber)

PEK (40% glass fiber, modified)

Carbon Filled PEK

PEK (20-30% carbon fiber)

PEK (30% carbon fiber)