PEK 30% Carbon Fiber Material Data Sheet

PEK 30% Carbon Fiber (Polyetherketone) Material Data Sheet

PEK 30% Carbon Fiber Overview

PEK 30% carbon fiber is a grade of polyetherketone (PEK), designated Polyetherketone (30% Carbon Fiber). This PEK 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEK parts in-house and inspects them before shipment.

PEK Designation

Polyetherketone (30% Carbon Fiber)
TradenamesArylmax, Avaspire, G-Paek, Victrex

PEK Typical uses

Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, housing for tire pressure sensors, valve spring discs, rollers, guides, gears, reciprocating components.

PEK 30% Carbon Fiber Composition detail

Polymer70  %
Carbon (fiber)30  %

PEK Physical properties

Density1.44–1.46g/cm3

PEK 30% Carbon Fiber Mechanical properties

Young’s modulus18.2–19.1GPa
Specific stiffness12.5–13.2MN.m/kg
Yield strength (elastic limit)158–174MPa
Tensile strength197–217MPa
Specific strength109–120kN.m/kg
Elongation1.4–1.61% strain
Compressive modulus18.2–19.1GPa
Compressive strength222–245MPa
Flexural modulus19.1–20.1GPa
Flexural strength (modulus of rupture)263–290MPa
Shear modulus6.84–7.18GPa
Bulk modulus17.8–18.7GPa
Poisson’s ratio0.323–0.336 
Shape factor8.9
Hardness – Vickers47–52HV
Hardness – Rockwell M100–110 
Hardness – Rockwell R121–133 
Elastic stored energy (springs)666–809kJ/m3
Fatigue strength at 10^7 cycles102–108MPa

PEK Impact & fracture properties

Fracture toughness5.82–7.33MPa.m0.5
Toughness (G)1.84–2.85kJ/m2
Impact strength, notched 23 °C8.18–9.9kJ/m2
Impact strength, notched -30 °C7.27–8.8kJ/m2
Impact strength, unnotched 23 °C50–60.5kJ/m2
Impact strength, unnotched -30 °C50–60.5kJ/m2

PEK 30% Carbon Fiber Thermal properties

Melting point317–341°C
Glass temperature182–200°C
Heat deflection temperature 0.45MPa315–375°C
Heat deflection temperature 1.8MPa306–365°C
Vicat softening point315–375°C
Maximum service temperature234–254°C
Minimum service temperature-47–-27°C
Thermal conductivity0.608–0.632W/m.°C
Specific heat capacity1340–1400J/kg.°C
Thermal expansion coefficient14–14.5µstrain/°C
Thermal shock resistance589–660°C
Thermal distortion resistance0.0424–0.0448MW/m

PEK Electrical properties

Electrical resistivity10000000–90000000µohm.cm
Electrical conductivity1.92e-6–1.72e-5%IACS
Galvanic potential0.14–0.22V

PEK Magnetic properties

Magnetic typeNon-magnetic

PEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3540–3630m/s
Mechanical loss coefficient (tan delta)0.00507–0.00525 

PEK Absorption & permeability

Water absorption @ 24 hrs0.1–0.2%

PEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingUnsuitable
Linear mold shrinkage0.2 – 0.8 %
Melt temperature334 – 429 °C
Molding pressure range68.8 – 138 MPa

PEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing

PEK Notes

PEK 30% Carbon Fiber Other notes
Endurance limit tested at 15 Hz