Home » PEK (Polyetherketone) » PEK Unfilled Grade Material Data Sheet
PEK Unfilled Grade (Polyetherketone) Material Data Sheet
PEK Unfilled Grade Overview
PEK unfilled grade is a grade of polyetherketone (PEK), designated Polyetherketone – unfilled. This PEK unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEK parts in-house and inspects them before shipment.
PEK Designation
Polyetherketone – unfilled Tradenames Arylmax, Avaspire, G-Paek, Peek-Classix, Victrex
PEK Typical uses
Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, housing for tire pressure sensors, valve spring discs, rollers, guides, gears, reciprocating components.
PEK Unfilled Grade Composition detail
PEK Physical properties
PEK Unfilled Grade Mechanical properties
Young’s modulus 3.59 – 4.1 GPa Specific stiffness 2.76 – 3.16 MN.m/kg Yield strength (elastic limit) 112 – 124 MPa Tensile strength 88.7 – 120 MPa Specific strength 86.1 – 95.4 kN.m/kg Elongation 20 – 53.8 % strain Compressive modulus 3.59 – 4.1 GPa Compressive strength 131 – 149 MPa Flexural modulus 3.55 – 4.1 GPa Flexural strength (modulus of rupture) 124 – 169 MPa Shear modulus 1.3 – 1.48 GPa Bulk modulus 5.41 – 5.91 GPa Poisson’s ratio 0.377 – 0.394 Shape factor 4.3 Hardness – Vickers 30 – 37 HV Hardness – Rockwell M 93 – 103 Hardness – Rockwell R 117 – 130 Elastic stored energy (springs) 1610 – 2040 kJ/m3 Fatigue strength at 10^7 cycles 32.7 – 67.3 MPa
PEK Impact & fracture properties
Fracture toughness 2.28 – 6.83 MPa.m0.5 Toughness (G) 1.64 – 9.99 kJ/m2 Impact strength, notched 23 °C 5.91 – 7.15 kJ/m2 Impact strength, notched -30 °C 5.91 – 7.15 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PEK Unfilled Grade Thermal properties
Melting point 368 – 394 °C Glass temperature 182 – 200 °C Heat deflection temperature 0.45MPa 225 – 306 °C Heat deflection temperature 1.8MPa 175 – 247 °C Vicat softening point 225 – 306 °C Maximum service temperature 179 – 214 °C Minimum service temperature -47 – -27 °C Thermal conductivity 0.286 – 0.31 W/m.°C Specific heat capacity 1450 – 1510 J/kg.°C Thermal expansion coefficient 72.4 – 79.6 µstrain/°C Thermal shock resistance 368 – 445 °C Thermal distortion resistance 0.00369 – 0.00417 MW/m
PEK Electrical properties
Electrical resistivity 3300000000000000000000 – 30000000000000000000000 µohm.cm Electrical conductivity 5.75e-21 – 5.22e-20 %IACS Dielectric constant (relative permittivity) 3.14 – 3.46 Dissipation factor (dielectric loss tangent) 0.00398 – 0.00477 Dielectric strength (dielectric breakdown) 13.4 – 14.5 MV/m Comparative tracking index 175 – 225 V
PEK Magnetic properties
Magnetic type Non-magnetic
PEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1660 – 1780 m/s Mechanical loss coefficient (tan delta) 0.00976 – 0.0111
PEK Absorption & permeability
Water absorption @ 24 hrs 0.09 – 0.11 %
PEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.8 – 1.5 % Melt temperature 379 – 430 °C Molding pressure range 68.8 – 138 MPa
PEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Good Flammability Self-extinguishing