Home » PEK (Polyetherketone) » PEK 40% Glass Fiber Material Data Sheet
PEK 40% Glass Fiber (Polyetherketone) Material Data Sheet
PEK 40% Glass Fiber Overview
PEK 40% glass fiber is a grade of polyetherketone (PEK), designated Polyetherketone (40% Glass Fiber). This PEK 40% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEK parts in-house and inspects them before shipment.
PEK Designation
Polyetherketone (40% Glass Fiber) Tradenames Avaspire
PEK Typical uses
Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, housing for tire pressure sensors, valve spring discs, rollers, guides, gears, reciprocating components.
PEK 40% Glass Fiber Composition detail
Polymer 60 % Glass (fiber) 40 %
PEK Physical properties
PEK 40% Glass Fiber Mechanical properties
Young’s modulus 12.8 – 13.4 GPa Specific stiffness 8.23 – 8.67 MN.m/kg Yield strength (elastic limit) 131 – 145 MPa Tensile strength 164 – 181 MPa Specific strength 84.5 – 93.6 kN.m/kg Elongation 1.86 – 2.15 % strain Compressive modulus 12.8 – 13.4 GPa Compressive strength 213 – 235 MPa Flexural modulus 14.1 – 14.8 GPa Flexural strength (modulus of rupture) 263 – 290 MPa Shear modulus 4.76 – 4.99 GPa Bulk modulus 13.7 – 14.3 GPa Poisson’s ratio 0.337 – 0.351 Shape factor 7.9 Hardness – Vickers 39 – 43 HV Hardness – Rockwell M 97 – 107 Hardness – Rockwell R 120 – 132 Elastic stored energy (springs) 657 – 801 kJ/m3 Fatigue strength at 10^7 cycles 60.5 – 78.7 MPa
PEK Impact & fracture properties
Fracture toughness 5.59 – 6.71 MPa.m0.5 Toughness (G) 2.4 – 3.41 kJ/m2 Impact strength, notched 23 °C 10 – 11 kJ/m2
PEK 40% Glass Fiber Thermal properties
Melting point 317 – 341 °C Glass temperature 182 – 200 °C Heat deflection temperature 0.45MPa 311 – 371 °C Heat deflection temperature 1.8MPa 298 – 356 °C Vicat softening point 311 – 371 °C Maximum service temperature 232 – 252 °C Minimum service temperature -47 – -27 °C Thermal conductivity 0.423 – 0.457 W/m.°C Specific heat capacity 1280 – 1330 J/kg.°C Thermal expansion coefficient 31.7 – 33.1 µstrain/°C Thermal shock resistance 307 – 344 °C Thermal distortion resistance 0.013 – 0.0142 MW/m
PEK Electrical properties
Electrical resistivity 3300000000000000000000 – 30000000000000000000000 µohm.cm Electrical conductivity 5.75e-21 – 5.22e-20 %IACS Dielectric constant (relative permittivity) 3.14 – 3.46 Dissipation factor (dielectric loss tangent) 0.00398 – 0.00477 Dielectric strength (dielectric breakdown) 15.9 – 17.2 MV/m Comparative tracking index 175 – 225 V
PEK Magnetic properties
Magnetic type Non-magnetic
PEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2870 – 2950 m/s Mechanical loss coefficient (tan delta) 0.0065 – 0.00671
PEK Absorption & permeability
Water absorption @ 24 hrs 0.0455 – 0.055 %
PEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.1 – 0.9 % Melt temperature 334 – 429 °C Molding pressure range 68.8 – 138 MPa
PEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Limited use Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Good Flammability Self-extinguishing
Modulus Metal Services
Manufacturing & Quality Services in Turkey