Home » PEK (Polyetherketone) » PEK 20% Glass Fiber Material Data Sheet
PEK 20% Glass Fiber (Polyetherketone) Material Data Sheet
PEK 20% Glass Fiber Overview
PEK 20% glass fiber is a grade of polyetherketone (PEK), designated Polyetherketone (20% Glass Fiber). This PEK 20% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEK parts in-house and inspects them before shipment.
PEK Designation
Polyetherketone (20% Glass Fiber) Tradenames G-Paek
PEK Typical uses
Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, housing for tire pressure sensors, valve spring discs, rollers, guides, gears, reciprocating components.
PEK 20% Glass Fiber Composition detail
Polymer 80 % Glass (fiber) 20 %
PEK Physical properties
PEK 20% Glass Fiber Mechanical properties
Young’s modulus 8.88 – 9.33 GPa Specific stiffness 6.12 – 6.44 MN.m/kg Yield strength (elastic limit) 130 – 143 MPa Tensile strength 162 – 179 MPa Specific strength 89.3 – 98.8 kN.m/kg Elongation 3.07 – 3.55 % strain Compressive modulus 8.88 – 9.33 GPa Compressive strength 156 – 172 MPa Flexural modulus 8.88 – 9.33 GPa Flexural strength (modulus of rupture) 229 – 252 MPa Shear modulus 3.27 – 3.44 GPa Bulk modulus 10.4 – 10.9 GPa Poisson’s ratio 0.35 – 0.365 Shape factor 6.3 Hardness – Vickers 39 – 43 HV Hardness – Rockwell M 95 – 105 Hardness – Rockwell R 119 – 131 Elastic stored energy (springs) 922 – 1130 kJ/m3 Fatigue strength at 10^7 cycles 59.8 – 77.8 MPa
PEK Impact & fracture properties
Fracture toughness 4.01 – 7.85 MPa.m0.5 Toughness (G) 1.92 – 6.22 kJ/m2 Impact strength, notched 23 °C 7.3 – 8.1 kJ/m2
PEK 20% Glass Fiber Thermal properties
Melting point 368 – 394 °C Glass temperature 182 – 200 °C Heat deflection temperature 0.45MPa 282 – 339 °C Heat deflection temperature 1.8MPa 225 – 276 °C Vicat softening point 282 – 339 °C Maximum service temperature 215 – 234 °C Minimum service temperature -47 – -27 °C Thermal conductivity 0.454 – 0.472 W/m.°C Specific heat capacity 1340 – 1400 J/kg.°C Thermal expansion coefficient 44.1 – 45.9 µstrain/°C Thermal shock resistance 314 – 353 °C Thermal distortion resistance 0.01 – 0.0106 MW/m
PEK Electrical properties
Electrical resistivity 3300000000000000000000 – 30000000000000000000000 µohm.cm Electrical conductivity 5.75e-21 – 5.22e-20 %IACS Dielectric constant (relative permittivity) 3.14 – 3.46 Dissipation factor (dielectric loss tangent) 0.00398 – 0.00477 Dielectric strength (dielectric breakdown) 13 – 15 MV/m Comparative tracking index 175 – 225 V
PEK Magnetic properties
Magnetic type Non-magnetic
PEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2470 – 2540 m/s Mechanical loss coefficient (tan delta) 0.00838 – 0.00867
PEK Absorption & permeability
Water absorption @ 24 hrs 0.06 – 0.08 %
PEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.818 – 0.99 % Melt temperature 344 – 430 °C Molding pressure range 68.8 – 138 MPa
PEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Limited use Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Good Flammability Self-extinguishing
Modulus Metal Services