Transparent PA Semi-Aromatic Type 6-3-T Amorphous Material Data Sheet
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Overview
Transparent PA semi-aromatic type 6-3-T amorphous is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (Semi-aromatic type 6-3-T, amorphous). This transparent PA semi-aromatic type 6-3-T amorphous material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Designation
Transparent polyamide (nylon) (Semi-aromatic type 6-3-T, amorphous) Tradenames Grivory, Selar, Trogamid, Durethan
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Typical uses
High-voltage switch casings, cable glands, battery seals, keys and push buttons, terminal strips, filter cups, metering devices, inspection glasses, flowmeters, liquid-level indicators, valve blocks, guide rails, coil body, toothbrush handle
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Composition detail
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Physical properties
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Mechanical properties
Young’s modulus 2.94 – 3.66 GPa Specific stiffness 2.64 – 3.29 MN.m/kg Yield strength (elastic limit) 63.7 – 79.5 MPa Tensile strength 101 – 124 MPa Specific strength 57.1 – 71.4 kN.m/kg Elongation 41 – 59 % strain Elongation at yield 4.58 – 8.7 % strain Compressive modulus 3.14 – 3.47 GPa Compressive strength 128 – 142 MPa Flexural modulus 3 – 3.6 GPa Flexural strength (modulus of rupture) 146 – 178 MPa Shear modulus 1.15 – 1.21 GPa Shear strength 60.8 – 74.3 MPa Bulk modulus 5.23 – 5.78 GPa Poisson’s ratio 0.38 – 0.4 Shape factor 5.1 Hardness – Vickers 20 – 23 HV Hardness – Rockwell M 154 – 170 Hardness – Rockwell R 154 – 170 Hardness – Shore D 91 – 95 Hardness – Shore A 98 – 100 Elastic stored energy (springs) 612 – 974 kJ/m3 Fatigue strength at 10^7 cycles 42.8 – 47.3 MPa Tear strength 159 – 169 N/mm
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Impact & fracture properties
Fracture toughness 3.89 – 4.3 MPa.m0.5 Toughness (G) 4.42 – 5.89 kJ/m2 Impact strength, notched 23 °C 6.8 – 13.2 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Thermal properties
Glass temperature 147 – 155 °C Heat deflection temperature 0.45MPa 137 – 142 °C Heat deflection temperature 1.8MPa 117 – 122 °C Vicat softening point 125 – 150 °C Maximum service temperature 80 – 90 °C Minimum service temperature -48 – -28 °C Thermal conductivity 0.14 – 0.16 W/m.°C Specific heat capacity 1400 – 1500 J/kg.°C Thermal expansion coefficient 53 – 60 µstrain/°C Thermal shock resistance 327 – 453 °C Thermal distortion resistance 0.00243 – 0.0029 MW/m
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Electrical properties
Electrical resistivity 2e20 – 5e21 µohm.cm Electrical conductivity 3.45e-20 – 8.62e-19 %IACS Dielectric constant (relative permittivity) 4 – 5.63 Dissipation factor (dielectric loss tangent) 0.0162 – 0.0426 Dielectric strength (dielectric breakdown) 20.7 – 35.3 MV/m Comparative tracking index 600 V
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Magnetic properties
Magnetic type Non-magnetic
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Optical, aesthetic and acoustic properties
Refractive index 1.56 – 1.57 Transparency Transparent Acoustic velocity 1620 – 1820 m/s Mechanical loss coefficient (tan delta) 0.0138 – 0.0153
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Absorption & permeability
Water absorption @ 24 hrs 1.5 – 2.4 % Water absorption @ sat 6.5 – 8.6 % Humidity absorption @ sat 2 – 2.7 % Water vapor transmission 0.776 – 1.04 g.mm/m².day Permeability (O2) 32 – 42.8 cm³.mm/m².day.atm
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.45 – 0.6 % Melt temperature 260 – 300 °C Mold temperature 60 – 80 °C Molding pressure range 80 – 160 MPa
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Limited use Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Unacceptable Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Notes
Transparent PA Semi-Aromatic Type 6-3-T Amorphous Other notes First commercialized by Dynamit Nobel, 1968.
Transparent Polyamide Grades
Transparent Polyamide Material Data Sheets
Unfilled Blends with Aliphatic PA, Low Tg Data sheet
Unfilled Cycloaliphatic, Microcrystalline Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, High Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Low Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Mid Tg Data sheet
Unfilled Semi-Aromatic Type 6-3-T, Amorphous You are here
Unfilled Semi-Aromatic Type 6I/6T, Amorphous Data sheet
Other Transparent Polyamide grades:
All Transparent Polyamide Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey