Home » PA (Polyamide / Nylon) » Transparent Polyamide (Transparent Nylon) » Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Material Data Sheet
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Material Data Sheet
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Overview
Transparent PA part-cycloaliphatic amorphous mid Tg is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, mid Tg). This transparent PA part-cycloaliphatic amorphous mid Tg material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Designation
Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, mid Tg) Tradenames Durethan, Grilamid, Grivory
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Typical uses
Viewing glasses, frames for safety glasses, electrical plugs, IR sensor housing, mobile phone housing, hearing aids, petrol filter, water pressure gauges, sight glasses, sanitary fittings and holders, baby bottles, catering containers, different transparent housings, extruded cable sheathing
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Composition detail
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Physical properties
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Mechanical properties
Young’s modulus 2.85 – 3.55 GPa Specific stiffness 2.66 – 3.32 MN.m/kg Yield strength (elastic limit) 56.7 – 70.8 MPa Tensile strength 56.7 – 69.3 MPa Specific strength 53 – 66.2 kN.m/kg Elongation 25.9 – 37.3 % strain Elongation at yield 12.2 – 23.3 % strain Compressive modulus 3.04 – 3.36 GPa Compressive strength 71.8 – 79.4 MPa Flexural modulus 2.91 – 3.49 GPa Flexural strength (modulus of rupture) 75.8 – 92.6 MPa Shear modulus 1.11 – 1.16 GPa Shear strength 34 – 41.6 MPa Bulk modulus 5.51 – 6.09 GPa Poisson’s ratio 0.392 – 0.408 Shape factor 5.32 Hardness – Vickers 18 – 20 HV Hardness – Rockwell M 119 – 131 Hardness – Rockwell R 119 – 131 Hardness – Brinell 94 – 117 HB Hardness – Shore D 82 – 86 Hardness – Shore A 90 – 100 Elastic stored energy (springs) 500 – 796 kJ/m3 Fatigue strength at 10^7 cycles 23.9 – 26.5 MPa Tear strength 155 – 171 N/mm
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Impact & fracture properties
Fracture toughness 3.87 – 4.28 MPa.m0.5 Toughness (G) 4.51 – 6.02 kJ/m2 Impact strength, notched 23 °C 7.89 – 15.3 kJ/m2 Impact strength, unnotched 23 °C 374 – 549 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Thermal properties
Glass temperature 155 – 168 °C Heat deflection temperature 0.45MPa 135 – 150 °C Heat deflection temperature 1.8MPa 115 – 136 °C Vicat softening point 139 – 154 °C Maximum service temperature 80 – 100 °C Minimum service temperature -48 – -28 °C Thermal conductivity 0.099 – 0.107 W/m.°C Specific heat capacity 1710 – 1780 J/kg.°C Thermal expansion coefficient 80 – 90 µstrain/°C Thermal shock resistance 200 – 276 °C Thermal distortion resistance 0.00113 – 0.0013 MW/m
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Electrical properties
Electrical resistivity 2e18 – 5e19 µohm.cm Electrical conductivity 3.45e-18 – 8.62e-17 %IACS Dielectric constant (relative permittivity) 3.91 – 5.51 Dissipation factor (dielectric loss tangent) 0.0207 – 0.0545 Dielectric strength (dielectric breakdown) 23.2 – 39.6 MV/m Comparative tracking index 600 V
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Magnetic properties
Magnetic type Non-magnetic
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Optical, aesthetic and acoustic properties
Refractive index 1.56 – 1.58 Transparency Transparent Acoustic velocity 1630 – 1820 m/s Mechanical loss coefficient (tan delta) 0.0141 – 0.0155
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Absorption & permeability
Water absorption @ 24 hrs 0.61 – 0.99 % Water absorption @ sat 2.4 – 3.2 % Humidity absorption @ sat 1.3 – 1.7 % Water vapor transmission 0.776 – 1.04 g.mm/m².day Permeability (O2) 32 – 42.8 cm³.mm/m².day.atm
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.6 – 0.75 % Melt temperature 260 – 290 °C Mold temperature 40 – 120 °C Molding pressure range 34.4 – 138 MPa
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Limited use Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Unacceptable Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Notes
Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Other notes Reference grades: Cristamid (Rilsan Clear) 1700, Grilamid TR55, Grilamid TR90
Transparent Polyamide Grades
Transparent Polyamide Material Data Sheets
Unfilled Blends with Aliphatic PA, Low Tg Data sheet
Unfilled Cycloaliphatic, Microcrystalline Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, High Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Low Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Mid Tg You are here
Unfilled Semi-Aromatic Type 6-3-T, Amorphous Data sheet
Unfilled Semi-Aromatic Type 6I/6T, Amorphous Data sheet
Other Transparent Polyamide grades:
All Transparent Polyamide Grades
Modulus Metal Services