Home » PA (Polyamide / Nylon) » Transparent Polyamide (Transparent Nylon) » Transparent PA Part-Cycloaliphatic Amorphous Low Tg Material Data Sheet
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Material Data Sheet
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Overview
Transparent PA part-cycloaliphatic amorphous low Tg is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, low Tg). This transparent PA part-cycloaliphatic amorphous low Tg material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Designation
Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, low Tg) Tradenames Durethan, Grilamid, Grivory
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Typical uses
Optics (glass frames), electricity / electronics, industry, sport
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Composition detail
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Physical properties
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Mechanical properties
Young’s modulus 1.74 – 2.16 GPa Specific stiffness 1.67 – 2.08 MN.m/kg Yield strength (elastic limit) 64.5 – 80.5 MPa Tensile strength 50.4 – 61.6 MPa Specific strength 62 – 77.4 kN.m/kg Elongation 124 – 178 % strain Elongation at yield 4.83 – 9.17 % strain Compressive modulus 1.85 – 2.05 GPa Compressive strength 63.8 – 70.6 MPa Flexural modulus 1.72 – 2.06 GPa Flexural strength (modulus of rupture) 65.9 – 80.5 MPa Shear modulus 0.676 – 0.71 GPa Shear strength 30.2 – 37 MPa Bulk modulus 3.32 – 3.67 GPa Poisson’s ratio 0.391 – 0.407 Shape factor 3.9 Hardness – Vickers 21 – 23 HV Hardness – Rockwell M 119 – 131 Hardness – Rockwell R 119 – 131 Hardness – Shore D 82 – 86 Hardness – Shore A 90 – 100 Elastic stored energy (springs) 1060 – 1690 kJ/m3 Fatigue strength at 10^7 cycles 21.3 – 23.5 MPa Tear strength 147 – 163 N/mm
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Impact & fracture properties
Fracture toughness 3.5 – 3.87 MPa.m0.5 Toughness (G) 6.06 – 8.06 kJ/m2 Impact strength, notched 23 °C 7.14 – 13.9 kJ/m2 Impact strength, notched -30 °C 7.88 – 17.1 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Thermal properties
Glass temperature 115 – 123 °C Heat deflection temperature 0.45MPa 98 – 103 °C Heat deflection temperature 1.8MPa 91 – 96 °C Vicat softening point 112 – 117 °C Maximum service temperature 80 – 100 °C Minimum service temperature -51 – -31 °C Thermal conductivity 0.0991 – 0.107 W/m.°C Specific heat capacity 1700 – 1770 J/kg.°C Thermal expansion coefficient 79 – 81 µstrain/°C Thermal shock resistance 399 – 541 °C Thermal distortion resistance 0.00124 – 0.00134 MW/m
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Electrical properties
Electrical resistivity 2e18 – 5e19 µohm.cm Electrical conductivity 3.45e-18 – 8.62e-17 %IACS Dielectric constant (relative permittivity) 3.91 – 5.51 Dissipation factor (dielectric loss tangent) 0.0207 – 0.0545 Dielectric strength (dielectric breakdown) 37 – 63 MV/m Comparative tracking index 600 V
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Magnetic properties
Magnetic type Non-magnetic
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Optical, aesthetic and acoustic properties
Refractive index 1.56 – 1.58 Transparency Transparent Acoustic velocity 1290 – 1440 m/s Mechanical loss coefficient (tan delta) 0.0183 – 0.0202
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Absorption & permeability
Water absorption @ 24 hrs 0.61 – 0.99 % Water absorption @ sat 2.4 – 3.1 % Humidity absorption @ sat 1 – 1.4 % Water vapor transmission 0.776 – 1.04 g.mm/m².day Permeability (O2) 32 – 42.8 cm³.mm/m².day.atm
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.6 – 0.75 % Melt temperature 245 – 275 °C Mold temperature 20 – 80 °C Molding pressure range 34.4 – 138 MPa
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Limited use Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Unacceptable Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Notes
Transparent PA Part-Cycloaliphatic Amorphous Low Tg Other notes Reference grade: Cristamid (Rilsan Clear) 1100
Transparent Polyamide Grades
Transparent Polyamide Material Data Sheets
Unfilled Blends with Aliphatic PA, Low Tg Data sheet
Unfilled Cycloaliphatic, Microcrystalline Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, High Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Low Tg You are here
Unfilled Part-Cycloaliphatic, Amorphous, Mid Tg Data sheet
Unfilled Semi-Aromatic Type 6-3-T, Amorphous Data sheet