Transparent PA Part-Cycloaliphatic Amorphous High Tg Material Data Sheet

Transparent PA Part-Cycloaliphatic Amorphous High Tg Material Data Sheet

Transparent PA Part-Cycloaliphatic Amorphous High Tg Overview

Transparent PA part-cycloaliphatic amorphous high Tg is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, high Tg). This transparent PA part-cycloaliphatic amorphous high Tg material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.

Transparent PA Part-Cycloaliphatic Amorphous High Tg Designation

Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, high Tg)
TradenamesDurethan, Grilamid, Grivory

Transparent PA Part-Cycloaliphatic Amorphous High Tg Typical uses

Applications requiring transparency, resistance to chemicals and high heat distortion temperature e.g. medicinal apparatus or parts in contact with hot oil.

Transparent PA Part-Cycloaliphatic Amorphous High Tg Composition detail

Polymer100  %

Transparent PA Part-Cycloaliphatic Amorphous High Tg Physical properties

Density1–1.02g/cm3

Transparent PA Part-Cycloaliphatic Amorphous High Tg Mechanical properties

Young’s modulus2.05–2.55GPa
Specific stiffness2.03–2.53MN.m/kg
Yield strength (elastic limit)66.8–83.3MPa
Tensile strength49.5–60.5MPa
Specific strength66.1–82.5kN.m/kg
Elongation41–59% strain
Elongation at yield4.14–7.86% strain
Compressive modulus2.19–2.42GPa
Compressive strength62.7–69.3MPa
Flexural modulus2.09–2.51GPa
Flexural strength (modulus of rupture)64.5–78.8MPa
Shear modulus0.799–0.84GPa
Shear strength29.7–36.3MPa
Bulk modulus3.75–4.15GPa
Poisson’s ratio0.387–0.403 
Shape factor4.2
Hardness – Vickers21–24HV
Hardness – Rockwell M122–135 
Hardness – Rockwell R122–135 
Hardness – Shore D83–87 
Hardness – Shore A90–100 
Elastic stored energy (springs)966–1530kJ/m3
Fatigue strength at 10^7 cycles20.9–23.1MPa
Tear strength158–174N/mm

Transparent PA Part-Cycloaliphatic Amorphous High Tg Impact & fracture properties

Fracture toughness3.62–4MPa.m0.5
Toughness (G)5.49–7.31kJ/m2
Impact strength, notched 23 °C4.08–7.92kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

Transparent PA Part-Cycloaliphatic Amorphous High Tg Thermal properties

Glass temperature186–194°C
Heat deflection temperature 0.45MPa162–167°C
Heat deflection temperature 1.8MPa147–152°C
Vicat softening point164–174°C
Maximum service temperature75–85°C
Minimum service temperature-48–-28°C
Thermal conductivity0.0995–0.108W/m.°C
Specific heat capacity1720–1790J/kg.°C
Thermal expansion coefficient79–81µstrain/°C
Thermal shock resistance350–475°C
Thermal distortion resistance0.00124–0.00135MW/m

Transparent PA Part-Cycloaliphatic Amorphous High Tg Electrical properties

Electrical resistivity2e18–5e19µohm.cm
Electrical conductivity3.45e-18–8.62e-17%IACS
Dielectric constant (relative permittivity)3.91–5.51 
Dissipation factor (dielectric loss tangent)0.0207–0.0545 
Dielectric strength (dielectric breakdown)23.7–40.3MV/m
Comparative tracking index600  V

Transparent PA Part-Cycloaliphatic Amorphous High Tg Magnetic properties

Magnetic typeNon-magnetic

Transparent PA Part-Cycloaliphatic Amorphous High Tg Optical, aesthetic and acoustic properties

Refractive index1.56–1.58 
TransparencyTransparent
Acoustic velocity1420–1590m/s
Mechanical loss coefficient (tan delta)0.0166–0.0183 

Transparent PA Part-Cycloaliphatic Amorphous High Tg Absorption & permeability

Water absorption @ 24 hrs1.5–2.5%
Water absorption @ sat3.4–4.6%
Humidity absorption @ sat1.3–1.8%
Water vapor transmission0.776–1.04g.mm/m².day
Permeability (O2)32–42.8cm³.mm/m².day.atm

Transparent PA Part-Cycloaliphatic Amorphous High Tg Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.85 – 0.95 %
Melt temperature260 – 290 °C
Mold temperature40 – 120 °C
Molding pressure range34.4 – 138 MPa

Transparent PA Part-Cycloaliphatic Amorphous High Tg Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisUnacceptable
Organic solventsLimited use
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySelf-extinguishing