Home » PA (Polyamide / Nylon) » Transparent Polyamide (Transparent Nylon) » Transparent PA Cycloaliphatic Microcrystalline Material Data Sheet
Transparent PA Cycloaliphatic Microcrystalline Material Data Sheet
Transparent PA Cycloaliphatic Microcrystalline Overview
Transparent PA cycloaliphatic microcrystalline is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (cycloaliphatic, microcrystalline). This transparent PA cycloaliphatic microcrystalline material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.
Transparent PA Cycloaliphatic Microcrystalline Designation
Transparent polyamide (nylon) (cycloaliphatic, microcrystalline) Tradenames Durethan, Grilamid, Grivory, Trogamid
Transparent PA Cycloaliphatic Microcrystalline Typical uses
Transparent PA Cycloaliphatic Microcrystalline Composition detail
Transparent PA Cycloaliphatic Microcrystalline Physical properties
Transparent PA Cycloaliphatic Microcrystalline Mechanical properties
Young’s modulus 1.26 – 1.58 GPa Specific stiffness 1.27 – 1.6 MN.m/kg Yield strength (elastic limit) 45.4 – 56.6 MPa Tensile strength 57.4 – 70.1 MPa Specific strength 45.8 – 57.2 kN.m/kg Elongation 41 – 59 % strain Elongation at yield 5.52 – 10.5 % strain Compressive modulus 1.35 – 1.49 GPa Compressive strength 72.7 – 80.3 MPa Flexural modulus 1.29 – 1.55 GPa Flexural strength (modulus of rupture) 76.8 – 93.9 MPa Shear modulus 0.489 – 0.514 GPa Shear strength 34.4 – 42.1 MPa Bulk modulus 2.68 – 2.96 GPa Poisson’s ratio 0.4 – 0.416 Shape factor 3.99 Hardness – Vickers 15 – 16 HV Hardness – Rockwell M 115 – 127 Hardness – Rockwell R 115 – 127 Hardness – Shore D 81 – 85 Hardness – Shore A 90 – 100 Elastic stored energy (springs) 721 – 1150 kJ/m3 Fatigue strength at 10^7 cycles 24.2 – 26.8 MPa Tear strength 148 – 164 N/mm
Transparent PA Cycloaliphatic Microcrystalline Impact & fracture properties
Fracture toughness 3.28 – 3.63 MPa.m0.5 Toughness (G) 7.28 – 9.78 kJ/m2 Impact strength, notched 23 °C 6.8 – 13.2 kJ/m2 Impact strength, notched -30 °C 6.93 – 15.1 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
Transparent PA Cycloaliphatic Microcrystalline Thermal properties
Melting point 224 – 242 °C Glass temperature 132 – 145 °C Heat deflection temperature 0.45MPa 120 – 126 °C Heat deflection temperature 1.8MPa 102 – 111 °C Vicat softening point 125 – 138 °C Maximum service temperature 197 – 214 °C Minimum service temperature -49 – -29 °C Thermal conductivity 0.25 – 0.28 W/m.°C Specific heat capacity 1750 – 1790 J/kg.°C Thermal expansion coefficient 88.9 – 91.1 µstrain/°C Thermal shock resistance 342 – 466 °C Thermal distortion resistance 0.00277 – 0.00312 MW/m
Transparent PA Cycloaliphatic Microcrystalline Electrical properties
Electrical resistivity 2e18 – 5e19 µohm.cm Electrical conductivity 3.45e-18 – 8.62e-17 %IACS Dielectric constant (relative permittivity) 3.91 – 5.51 Dissipation factor (dielectric loss tangent) 0.0207 – 0.0545 Dielectric strength (dielectric breakdown) 24 – 40.8 MV/m Comparative tracking index 600 V
Transparent PA Cycloaliphatic Microcrystalline Magnetic properties
Magnetic type Non-magnetic
Transparent PA Cycloaliphatic Microcrystalline Optical, aesthetic and acoustic properties
Refractive index 1.51 – 1.52 Transparency Optical quality Acoustic velocity 1130 – 1270 m/s Mechanical loss coefficient (tan delta) 0.0211 – 0.0233
Transparent PA Cycloaliphatic Microcrystalline Absorption & permeability
Water absorption @ 24 hrs 0.59 – 0.96 % Water absorption @ sat 2.6 – 3.4 % Humidity absorption @ sat 0.94 – 1.3 % Water vapor transmission 0.834 – 0.964 g.mm/m².day Permeability (O2) 34.4 – 39.8 cm³.mm/m².day.atm
Transparent PA Cycloaliphatic Microcrystalline Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.4 – 0.8 % Melt temperature 280 – 300 °C Mold temperature 15 – 90 °C Molding pressure range 80 – 160 MPa
Transparent PA Cycloaliphatic Microcrystalline Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Limited use Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Unacceptable Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
Transparent PA Cycloaliphatic Microcrystalline Notes
Transparent PA Cycloaliphatic Microcrystalline Other notes Reference grades: Rilsan Clear, Trogamid CX 7323
Transparent Polyamide Grades
Transparent Polyamide Material Data Sheets
Unfilled Blends with Aliphatic PA, Low Tg Data sheet
Unfilled Cycloaliphatic, Microcrystalline You are here
Unfilled Part-Cycloaliphatic, Amorphous, High Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Low Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Mid Tg Data sheet
Unfilled Semi-Aromatic Type 6-3-T, Amorphous Data sheet
Unfilled Semi-Aromatic Type 6I/6T, Amorphous Data sheet
Other Transparent Polyamide grades:
All Transparent Polyamide Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey