Transparent PA Blends with Aliphatic PA Low Tg Material Data Sheet

Transparent PA Blends with Aliphatic PA Low Tg Material Data Sheet

Transparent PA Blends with Aliphatic PA Low Tg Overview

Transparent PA blends with aliphatic PA low Tg is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (Blends with aliphatic PA, low Tg). This transparent PA blends with aliphatic PA low Tg material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.

Transparent PA Blends with Aliphatic PA Low Tg Designation

Transparent polyamide (nylon) (Blends with aliphatic PA, low Tg)
TradenamesGrivory, Selar, Trogamid, Grilamid

Transparent PA Blends with Aliphatic PA Low Tg Typical uses

High quality spectacle frames, hearing aids, transparent housings

Transparent PA Blends with Aliphatic PA Low Tg Composition detail

Polymer100  %

Transparent PA Blends with Aliphatic PA Low Tg Physical properties

Density1.01–1.03g/cm3

Transparent PA Blends with Aliphatic PA Low Tg Mechanical properties

Young’s modulus1.54–1.91GPa
Specific stiffness1.51–1.87MN.m/kg
Yield strength (elastic limit)56.7–70.8MPa
Tensile strength36–44MPa
Specific strength55.6–69.4kN.m/kg
Elongation41–59% strain
Elongation at yield4.14–7.86% strain
Compressive modulus1.64–1.81GPa
Compressive strength45.6–50.4MPa
Flexural modulus1.57–1.88GPa
Flexural strength (modulus of rupture)43.2–52.8MPa
Shear modulus0.597–0.628GPa
Shear strength21.6–26.4MPa
Bulk modulus2.97–3.28GPa
Poisson’s ratio0.392–0.408 
Shape factor3.9
Hardness – Vickers18–20HV
Hardness – Rockwell M106–117 
Hardness – Rockwell R106–117 
Hardness – Brinell94–117HB
Hardness – Shore D79–82 
Hardness – Shore A90–100 
Elastic stored energy (springs)928–1480kJ/m3
Fatigue strength at 10^7 cycles15.2–16.8MPa
Tear strength151–164N/mm

Transparent PA Blends with Aliphatic PA Low Tg Impact & fracture properties

Fracture toughness3.42–3.77MPa.m0.5
Toughness (G)6.53–8.66kJ/m2
Impact strength, notched 23 °C7.99–15.5kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

Transparent PA Blends with Aliphatic PA Low Tg Thermal properties

Glass temperature93–110°C
Heat deflection temperature 0.45MPa85–90°C
Heat deflection temperature 1.8MPa75–80°C
Vicat softening point96–101°C
Maximum service temperature75–85°C
Minimum service temperature-54–-34°C
Thermal conductivity0.099–0.107W/m.°C
Specific heat capacity1680–1750J/kg.°C
Thermal expansion coefficient70–110µstrain/°C
Thermal shock resistance323–548°C
Thermal distortion resistance9.34e-4–0.00148MW/m

Transparent PA Blends with Aliphatic PA Low Tg Electrical properties

Electrical resistivity2e18–5e19µohm.cm
Electrical conductivity3.45e-18–8.62e-17%IACS
Dielectric constant (relative permittivity)3.91–5.51 
Dissipation factor (dielectric loss tangent)0.0207–0.0545 
Dielectric strength (dielectric breakdown)24.2–41.3MV/m
Comparative tracking index600  V

Transparent PA Blends with Aliphatic PA Low Tg Magnetic properties

Magnetic typeNon-magnetic

Transparent PA Blends with Aliphatic PA Low Tg Optical, aesthetic and acoustic properties

Refractive index1.56–1.58 
TransparencyTransparent
Acoustic velocity1230–1370m/s
Mechanical loss coefficient (tan delta)0.0191–0.0212 

Transparent PA Blends with Aliphatic PA Low Tg Absorption & permeability

Water absorption @ 24 hrs0.51–0.84%
Water absorption @ sat2.3–3%
Humidity absorption @ sat0.96–1.3%
Water vapor transmission0.776–1.04g.mm/m².day
Permeability (O2)32–42.8cm³.mm/m².day.atm

Transparent PA Blends with Aliphatic PA Low Tg Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.45 – 0.7 %
Melt temperature270 – 300 °C
Mold temperature60 – 80 °C
Molding pressure range80 – 160 MPa

Transparent PA Blends with Aliphatic PA Low Tg Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisUnacceptable
Organic solventsLimited use
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning

Transparent PA Blends with Aliphatic PA Low Tg Notes

Transparent PA Blends with Aliphatic PA Low Tg Other notes
Reference grades: Grilamid TR55 LX, LY, LZ ; Trogamid BX 7304