PA612 (nylon 612) resists heat better than PA610. Compared with PA6 and PA66 it absorbs less water, keeps its dimensions and electrical properties better and stays tough at lower temperatures. Its mold shrinkage is lower than PA6, PA66 and PA610, and in moist conditions its creep resistance is slightly better than PA66.
PA612 Limitations
Strength and heat distortion temperature are below PA66, and it costs more than PA6 and PA66.
PA612 Designation
PA612, also written 6.12 or 6/12.
Typical Uses of PA612
Mechanical parts, zips, filaments, coverings and coatings that need abrasion resistance.
PA612 Compositional Summary
(NH(CH2)6-NH-CO-(CH2)10-CO)n
Material family
Plastic (thermoplastic, semi-crystalline)
Base material
PA612 (Polyamide / nylon 612)
CAS number
26098-55-5
PA612 Processing Properties
Joining
Ultrasonic welding is harder than with PA6 or PA66.
PA612 Parts from Turkey
Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.