PA612 30% Glass Fiber Flame Retarded Material Data Sheet

PA612 30% Glass Fiber Flame Retarded (Polyamide 612) Material Data Sheet

PA612 30% Glass Fiber Flame Retarded Overview

PA612 30% glass fiber flame retarded is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 30% Glass Fiber, Flame Retarded). This PA612 30% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.

PA612 30% Glass Fiber Flame Retarded Designation

Polyamide (Nylon) (Type 612, 30% Glass Fiber, Flame Retarded)
TradenamesAkromid, Edgetek, Grilamid, Technyl, Ultramid, Zytel

PA612 30% Glass Fiber Flame Retarded Typical uses

Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.

PA612 30% Glass Fiber Flame Retarded Composition detail

Polymer55–65%
Flame retardant5–15%
Glass (fiber)30  %

PA612 30% Glass Fiber Flame Retarded Physical properties

Density1.29–1.31g/cm3

PA612 30% Glass Fiber Flame Retarded Mechanical properties

Young’s modulus8.96–11.2GPa
Specific stiffness6.89–8.62MN.m/kg
Yield strength (elastic limit)125–155MPa
Tensile strength126–154MPa
Specific strength96.1–119kN.m/kg
Elongation2.31–3.32% strain
Elongation at yield1.94–3.69% strain
Compressive modulus9.57–10.6GPa
Compressive strength160–176MPa
Flexural modulus7.88–9.44GPa
Flexural strength (modulus of rupture)188–229MPa
Shear modulus3.59–3.77GPa
Shear strength75.6–92.4MPa
Bulk modulus12.1–13.3GPa
Poisson’s ratio0.354–0.368 
Shape factor6.59
Hardness – Vickers40–44HV
Hardness – Rockwell M170–188 
Hardness – Rockwell R170–188 
Hardness – Shore D95–99 
Elastic stored energy (springs)770–1210kJ/m3
Fatigue strength at 10^7 cycles53.2–58.8MPa

PA612 30% Glass Fiber Flame Retarded Impact & fracture properties

Fracture toughness4.88–5.39MPa.m0.5
Toughness (G)2.27–3.04kJ/m2
Impact strength, notched 23 °C10.2–19.8kJ/m2
Impact strength, notched -30 °C6.3–13.7kJ/m2
Impact strength, unnotched 23 °C64.8–95.2kJ/m2
Impact strength, unnotched -30 °C42–63kJ/m2

PA612 30% Glass Fiber Flame Retarded Thermal properties

Melting point195–217°C
Glass temperature40–52°C
Heat deflection temperature 0.45MPa182–228°C
Heat deflection temperature 1.8MPa174–220°C
Maximum service temperature90–120°C
Minimum service temperature-127–-107°C
Thermal conductivity0.436–0.453W/m.°C
Specific heat capacity1340–1400J/kg.°C
Thermal expansion coefficient48.9–49.9µstrain/°C
Thermal shock resistance242–327°C
Thermal distortion resistance0.00879–0.00919MW/m

PA612 30% Glass Fiber Flame Retarded Electrical properties

Electrical resistivity2.73e21–6.83e22µohm.cm
Electrical conductivity2.52e-21–6.32e-20%IACS
Dielectric constant (relative permittivity)4.57–6.44 
Dissipation factor (dielectric loss tangent)0.0223–0.0587 
Dielectric strength (dielectric breakdown)20.4–34.7MV/m
Comparative tracking index600  V

PA612 30% Glass Fiber Flame Retarded Magnetic properties

Magnetic typeNon-magnetic

PA612 30% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2620–2940m/s
Mechanical loss coefficient (tan delta)0.00854–0.00944 

PA612 30% Glass Fiber Flame Retarded Absorption & permeability

Water absorption @ 24 hrs0.11–0.19%
Water absorption @ sat1.7–2.2%
Humidity absorption @ sat0.7–0.95%

PA612 30% Glass Fiber Flame Retarded Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.2 – 0.5 %
Melt temperature213 – 288 °C
Mold temperature30 – 60 °C
Molding pressure range27.5 – 138 MPa

PA612 30% Glass Fiber Flame Retarded Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySelf-extinguishing