PA612 30% Glass Fiber 15% PTFE Lubricated (Polyamide 612) Material Data Sheet
PA612 30% Glass Fiber 15% PTFE Lubricated Overview
PA612 30% glass fiber 15% PTFE lubricated is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 15% PTFE/30% Glass Fiber Lubricated). This PA612 30% glass fiber 15% PTFE lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.
PA612 30% Glass Fiber 15% PTFE Lubricated Designation
Polyamide (Nylon) (Type 612, 15% PTFE/30% Glass Fiber Lubricated) Tradenames Inlube, LNP Lubricomp, Tribocomp
PA612 30% Glass Fiber 15% PTFE Lubricated Typical uses
Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.
PA612 30% Glass Fiber 15% PTFE Lubricated Composition detail
Polymer 55 % PTFE (lubricant) 15 % Glass (fiber) 30 %
PA612 30% Glass Fiber 15% PTFE Lubricated Physical properties
PA612 30% Glass Fiber 15% PTFE Lubricated Mechanical properties
Young’s modulus 6.33 – 7.9 GPa Specific stiffness 4.44 – 5.55 MN.m/kg Yield strength (elastic limit) 122 – 152 MPa Tensile strength 123 – 150 MPa Specific strength 85.6 – 107 kN.m/kg Elongation 2.98 – 4.29 % strain Elongation at yield 2.51 – 4.76 % strain Compressive modulus 6.76 – 7.47 GPa Compressive strength 156 – 172 MPa Flexural modulus 5.67 – 6.79 GPa Flexural strength (modulus of rupture) 183 – 224 MPa Shear modulus 2.54 – 2.67 GPa Shear strength 73.9 – 90.3 MPa Bulk modulus 8.54 – 9.43 GPa Poisson’s ratio 0.354 – 0.368 Shape factor 5.42 Hardness – Vickers 39 – 43 HV Hardness – Rockwell M 169 – 186 Hardness – Rockwell R 169 – 186 Hardness – Shore D 95 – 99 Elastic stored energy (springs) 1040 – 1650 kJ/m3 Fatigue strength at 10^7 cycles 52 – 57.5 MPa
PA612 30% Glass Fiber 15% PTFE Lubricated Impact & fracture properties
Fracture toughness 4.55 – 5.03 MPa.m0.5 Toughness (G) 2.8 – 3.74 kJ/m2 Impact strength, notched 23 °C 10.2 – 19.8 kJ/m2 Impact strength, notched -30 °C 6.3 – 13.7 kJ/m2 Impact strength, unnotched 23 °C 64.8 – 95.2 kJ/m2 Impact strength, unnotched -30 °C 42 – 63 kJ/m2
PA612 30% Glass Fiber 15% PTFE Lubricated Thermal properties
Melting point 195 – 217 °C Glass temperature 40 – 52 °C Heat deflection temperature 0.45MPa 199 – 247 °C Heat deflection temperature 1.8MPa 174 – 220 °C Maximum service temperature 90 – 120 °C Minimum service temperature -127 – -107 °C Thermal conductivity 0.436 – 0.453 W/m.°C Specific heat capacity 1350 – 1410 J/kg.°C Thermal expansion coefficient 31.7 – 33.1 µstrain/°C Thermal shock resistance 510 – 693 °C Thermal distortion resistance 0.0133 – 0.0141 MW/m
PA612 30% Glass Fiber 15% PTFE Lubricated Electrical properties
Electrical resistivity 2.73e21 – 6.83e22 µohm.cm Electrical conductivity 2.52e-21 – 6.32e-20 %IACS Dielectric constant (relative permittivity) 4.57 – 6.44 Dissipation factor (dielectric loss tangent) 0.0223 – 0.0587 Dielectric strength (dielectric breakdown) 20.4 – 34.7 MV/m Comparative tracking index 600 V
PA612 30% Glass Fiber 15% PTFE Lubricated Magnetic properties
Magnetic type Non-magnetic
PA612 30% Glass Fiber 15% PTFE Lubricated Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2100 – 2360 m/s Mechanical loss coefficient (tan delta) 0.0101 – 0.0111
PA612 30% Glass Fiber 15% PTFE Lubricated Absorption & permeability
Water absorption @ 24 hrs 0.3 – 0.48 % Water absorption @ sat 1.3 – 1.7 % Humidity absorption @ sat 0.55 – 0.75 %
PA612 30% Glass Fiber 15% PTFE Lubricated Processing properties
Polymer injection molding Excellent Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 0.2 – 0.3 % Melt temperature 213 – 288 °C Mold temperature 30 – 60 °C Molding pressure range 27.5 – 138 MPa
PA612 30% Glass Fiber 15% PTFE Lubricated Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
PA612 Grades
PA612 Glass and PTFE Filled Material Data Sheets
Glass 30% Glass Fiber, 15% PTFE, Lubricated You are here
All PA612 Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey