PA612 30-35% Glass Fiber Material Data Sheet

PA612 30-35% Glass Fiber (Polyamide 612) Material Data Sheet

PA612 30-35% Glass Fiber Overview

PA612 30-35% glass fiber is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 30-35% Glass Fiber). This PA612 30-35% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.

PA612 30-35% Glass Fiber Designation

Polyamide (Nylon) (Type 612, 30-35% Glass Fiber)
TradenamesBadamid, Grilamid, LNP Thermocomp, Nybex, Schulamid

PA612 30-35% Glass Fiber Typical uses

Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.

PA612 30-35% Glass Fiber Composition detail

Polymer65–70%
Glass (fiber)30–35%

PA612 30-35% Glass Fiber Physical properties

Density1.32–1.34g/cm3

PA612 30-35% Glass Fiber Mechanical properties

Young’s modulus7.08–8.82GPa
Specific stiffness5.32–6.63MN.m/kg
Yield strength (elastic limit)125–155MPa
Tensile strength126–154MPa
Specific strength94–117kN.m/kg
Elongation2.54–3.66% strain
Elongation at yield2.14–4.06% strain
Compressive modulus7.55–8.35GPa
Compressive strength160–176MPa
Flexural modulus6.37–7.63GPa
Flexural strength (modulus of rupture)188–229MPa
Shear modulus2.83–2.98GPa
Shear strength75.6–92.4MPa
Bulk modulus9.54–10.5GPa
Poisson’s ratio0.354–0.368 
Shape factor5.7
Hardness – Vickers40–44HV
Hardness – Rockwell M170–188 
Hardness – Rockwell R170–188 
Hardness – Shore D95–99 
Elastic stored energy (springs)977–1540kJ/m3
Fatigue strength at 10^7 cycles53.2–58.8MPa

PA612 30-35% Glass Fiber Impact & fracture properties

Fracture toughness4.65–5.14MPa.m0.5
Toughness (G)2.62–3.49kJ/m2
Impact strength, notched 23 °C8.16–15.8kJ/m2
Impact strength, notched -30 °C6.3–13.7kJ/m2
Impact strength, unnotched 23 °C64.8–95.2kJ/m2
Impact strength, unnotched -30 °C42–63kJ/m2

PA612 30-35% Glass Fiber Thermal properties

Melting point213–217°C
Glass temperature40–52°C
Heat deflection temperature 0.45MPa204–221°C
Heat deflection temperature 1.8MPa199–218°C
Maximum service temperature90–120°C
Minimum service temperature-127–-107°C
Thermal conductivity0.411–0.444W/m.°C
Specific heat capacity1420–1480J/kg.°C
Thermal expansion coefficient51.2–52.2µstrain/°C
Thermal shock resistance293–396°C
Thermal distortion resistance0.00794–0.0086MW/m

PA612 30-35% Glass Fiber Electrical properties

Electrical resistivity2.73e21–6.83e22µohm.cm
Electrical conductivity2.52e-21–6.32e-20%IACS
Dielectric constant (relative permittivity)4.57–6.44 
Dissipation factor (dielectric loss tangent)0.0223–0.0587 
Dielectric strength (dielectric breakdown)20.4–34.7MV/m
Comparative tracking index600  V

PA612 30-35% Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PA612 30-35% Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2300–2580m/s
Mechanical loss coefficient (tan delta)0.0095–0.0105 

PA612 30-35% Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.23–0.37%
Water absorption @ sat1.5–2.1%
Humidity absorption @ sat0.59–0.8%

PA612 30-35% Glass Fiber Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.2 – 0.5 %
Melt temperature192 – 288 °C
Mold temperature30 – 60 °C
Molding pressure range27.5 – 138 MPa

PA612 30-35% Glass Fiber Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning