Home » PA (Polyamide / Nylon) » PA612 (Polyamide 612 / Nylon 612) » PA612 Carbon and PTFE Filled Grades » PA612 30% Carbon Fiber 10% PTFE Lubricated Material Data Sheet
PA612 30% Carbon Fiber 10% PTFE Lubricated (Polyamide 612) Material Data Sheet
PA612 30% Carbon Fiber 10% PTFE Lubricated Overview
PA612 30% carbon fiber 10% PTFE lubricated is a grade of polyamide 612 (PA612, nylon 612), designated Polyamide (Nylon) (Type 612, 30% carbon fiber, 10% PTFE, lubricated). This PA612 30% carbon fiber 10% PTFE lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.
PA612 30% Carbon Fiber 10% PTFE Lubricated Designation
Polyamide (Nylon) (Type 612, 30% carbon fiber, 10% PTFE, lubricated) Tradenames Inlube, Lubrione, Tribocomp
PA612 30% Carbon Fiber 10% PTFE Lubricated Typical uses
Mechanical parts, zips, filaments, coverings and coatings requiring abrasion resistance.
PA612 30% Carbon Fiber 10% PTFE Lubricated Composition detail
Polymer 60 % PTFE (lubricant) 10 % Carbon (fiber) 30 %
PA612 30% Carbon Fiber 10% PTFE Lubricated Physical properties
PA612 30% Carbon Fiber 10% PTFE Lubricated Mechanical properties
Young’s modulus 16 – 19.9 GPa Specific stiffness 12.1 – 15 MN.m/kg Yield strength (elastic limit) 174 – 217 MPa Tensile strength 176 – 215 MPa Specific strength 131 – 164 kN.m/kg Elongation 1.83 – 2.63 % strain Elongation at yield 1.54 – 2.92 % strain Compressive modulus 17.1 – 18.9 GPa Compressive strength 223 – 246 MPa Flexural modulus 13.8 – 16.5 GPa Flexural strength (modulus of rupture) 268 – 328 MPa Shear modulus 6.54 – 6.88 GPa Shear strength 106 – 129 MPa Bulk modulus 17.6 – 19.4 GPa Poisson’s ratio 0.325 – 0.338 Shape factor 7.73 Hardness – Vickers 56 – 62 HV Hardness – Rockwell M 184 – 204 Hardness – Rockwell R 184 – 204 Hardness – Shore D 98 – 102 Elastic stored energy (springs) 839 – 1330 kJ/m3 Fatigue strength at 10^7 cycles 74.3 – 82.1 MPa
PA612 30% Carbon Fiber 10% PTFE Lubricated Impact & fracture properties
Fracture toughness 5.48 – 6.06 MPa.m0.5 Toughness (G) 1.61 – 2.15 kJ/m2 Impact strength, notched 23 °C 10.2 – 19.8 kJ/m2 Impact strength, notched -30 °C 6.3 – 13.7 kJ/m2 Impact strength, unnotched 23 °C 64.8 – 95.2 kJ/m2 Impact strength, unnotched -30 °C 42 – 63 kJ/m2
PA612 30% Carbon Fiber 10% PTFE Lubricated Thermal properties
Melting point 195 – 217 °C Glass temperature 40 – 52 °C Heat deflection temperature 0.45MPa 201 – 249 °C Heat deflection temperature 1.8MPa 176 – 222 °C Maximum service temperature 90 – 120 °C Minimum service temperature -127 – -107 °C Thermal conductivity 0.57 – 0.593 W/m.°C Specific heat capacity 1450 – 1510 J/kg.°C Thermal expansion coefficient 30.1 – 30.7 µstrain/°C Thermal shock resistance 308 – 417 °C Thermal distortion resistance 0.0187 – 0.0196 MW/m
PA612 30% Carbon Fiber 10% PTFE Lubricated Electrical properties
Electrical resistivity 100000 – 1e7 µohm.cm Electrical conductivity 1.72e-5 – 0.00172 %IACS Galvanic potential 0.14 – 0.22 V
PA612 30% Carbon Fiber 10% PTFE Lubricated Magnetic properties
Magnetic type Non-magnetic
PA612 30% Carbon Fiber 10% PTFE Lubricated Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3470 – 3880 m/s Mechanical loss coefficient (tan delta) 0.00645 – 0.00713
PA612 30% Carbon Fiber 10% PTFE Lubricated Absorption & permeability
Water absorption @ 24 hrs 0.3 – 0.48 % Water absorption @ sat 1.3 – 1.7 % Humidity absorption @ sat 0.55 – 0.75 %
PA612 30% Carbon Fiber 10% PTFE Lubricated Processing properties
Polymer injection molding Limited use Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 0.118 – 0.143 % Melt temperature 213 – 288 °C Mold temperature 30 – 60 °C Molding pressure range 27.5 – 138 MPa
PA612 30% Carbon Fiber 10% PTFE Lubricated Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
PA612 Grades
PA612 Carbon and PTFE Filled Material Data Sheets
Carbon 30% Carbon Fiber, 10% PTFE, Lubricated You are here
All PA612 Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey