AISI 1040 Water Quenched & Tempered at 650°C Material Data Sheet
AISI 1040 Water Quenched & Tempered at 650°C Overview
| AISI 1040 water quenched tempered 650°C is AISI 1040 medium carbon steel (UNS G10400) in the water quenched & tempered at 650°C condition. This AISI 1040 water quenched tempered 650°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 1040 conditions in our AISI 1040 yield, tensile and hardness comparison. Looking for AISI 1040 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1040 steel parts in-house and inspects them before shipment. |
AISI 1040 Water Quenched & Tempered at 650°C Designation
| AISI 1040 | |
| Condition | Tempered at 650°C & water quenched |
| UNS number | G10400 |
| US name | ASTM G10420, ASTM 1042, ASTM 1040, ASME G10400, ASME G10390, ASME 1039 |
| EN name | ~HS40 |
| ISO name | ~CE40E4 |
| JIS (Japanese) name | ~STKM16C, ~STKM16A |
AISI 1040 Water Quenched & Tempered at 650°C Typical uses
| Heavy duty shafts, axles, crankshafts, couplings, gears (if given a hardening treatment) |
AISI 1040 Water Quenched & Tempered at 650°C Composition detail
| C (carbon) | 0.37 | – | 0.44 | % |
| Fe (iron) | 98.6 | – | 99 | % |
| Mn (manganese) | 0.6 | – | 0.9 | % |
| P (phosphorus) | 0 | – | 0.04 | % |
| S (sulfur) | 0 | – | 0.05 | % |
AISI 1040 Water Quenched & Tempered at 650°C Physical properties
| Density | 7.8 | – | 7.9 | g/cm3 |
AISI 1040 Water Quenched & Tempered at 650°C Mechanical properties
| Young’s modulus | 208 | – | 216 | GPa |
| Specific stiffness | 26.5 | – | 27.5 | MN.m/kg |
| Yield strength (elastic limit) | 455 | – | 550 | MPa |
| Tensile strength | 600 | – | 740 | MPa |
| Specific strength | 58 | – | 70.1 | kN.m/kg |
| Elongation | 22 | – | 34 | % strain |
| Compressive strength | 455 | – | 550 | MPa |
| Flexural modulus | 208 | – | 216 | GPa |
| Flexural strength (modulus of rupture) | 455 | – | 550 | MPa |
| Shear modulus | 80 | – | 85 | GPa |
| Bulk modulus | 161 | – | 176 | GPa |
| Poisson’s ratio | 0.285 | – | 0.295 | |
| Shape factor | 48 | |||
| Hardness – Vickers | 188 | – | 228 | HV |
| Elastic stored energy (springs) | 492 | – | 708 | kJ/m3 |
| Fatigue strength at 10^7 cycles | 299 | – | 347 | MPa |
| Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles | 259 | – | 401 | MPa |
AISI 1040 Water Quenched & Tempered at 650°C Impact & fracture properties
| Fracture toughness | 38 | – | 60 | MPa.m0.5 |
| Toughness (G) | 7.11 | – | 16.3 | kJ/m2 |
AISI 1040 Water Quenched & Tempered at 650°C Thermal properties
| Melting point | 1430 | – | 1510 | °C |
| Maximum service temperature | 323 | – | 350 | °C |
| Minimum service temperature | -58 | – | -28 | °C |
| Thermal conductivity | 50 | – | 54 | W/m.°C |
| Specific heat capacity | 465 | – | 505 | J/kg.°C |
| Thermal expansion coefficient | 10.5 | – | 12 | µstrain/°C |
| Thermal shock resistance | 187 | – | 236 | °C |
| Thermal distortion resistance | 4.29 | – | 5 | MW/m |
| Latent heat of fusion | 270 | – | 275 | kJ/kg |
AISI 1040 Water Quenched & Tempered at 650°C Electrical properties
| Electrical resistivity | 16 | – | 19 | µohm.cm |
| Electrical conductivity | 9.07 | – | 10.8 | %IACS |
| Galvanic potential | -0.52 | – | -0.44 | V |
AISI 1040 Water Quenched & Tempered at 650°C Magnetic properties
| Magnetic type | Magnetic |
AISI 1040 Water Quenched & Tempered at 650°C Optical, aesthetic and acoustic properties
| Transparency | Opaque | |||
| Acoustic velocity | 5140 | – | 5250 | m/s |
| Mechanical loss coefficient (tan delta) | 6.5e-4 | – | 8.1e-4 | |
AISI 1040 Water Quenched & Tempered at 650°C Processing properties
| Metal casting | Unsuitable |
| Metal cold forming | Acceptable |
| Metal hot forming | Acceptable |
| Metal press forming | Acceptable |
| Metal deep drawing | Limited use |
| Machining speed | 25 m/min |
| Weldability Notes: Preheating and post weld heat treatments are required | Good |
| Carbon equivalency | 0.47 – 0.59 |
AISI 1040 Water Quenched & Tempered at 650°C Durability
| Water (fresh) | Acceptable |
| Water (salt) | Limited use |
| Weak acids | Limited use |
| Strong acids | Unacceptable |
| Weak alkalis | Acceptable |
| Strong alkalis | Limited use |
| Organic solvents | Excellent |
| Oxidation at 500C | Acceptable |
| UV radiation (sunlight) | Excellent |
| Galling resistance (adhesive wear) Notes: Can be used for gears only if hardened. Aluminum bronze is the most suitable mating material to minimize galling. | Limited use |
| Flammability | Non-flammable |
AISI 1040 Water Quenched & Tempered at 650°C Corrosion resistance
| Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Nitrate, hydroxide, carbonate, ammonia | Not susceptible |
AISI 1040 Water Quenched & Tempered at 650°C Notes
| AISI 1040 Water Quenched & Tempered at 650°C Other notes |
| Responds to heat treatment and can be flame or induction hardened to 500 HV for gears and for good wear resistance. |
AISI 1040 Water Quenched & Tempered at 650°C Standards with similar compositions
| India: 40C8 to IS 1570/2/1, 45C8 to IS 1570/2/1, C40 to IS 1570/2/1, C45 to IS 1570/2/1, IS 6902 to IS 6902 |
| Mexico: 1038 to NMX-B-301, 1039 to NMX-B-301, 1040 to NMX-B-203-SCFI, 1040 to NMX-B-301, 1042 to NMX-B-301, 1043 to NMX-B-301 |
| Pan America: 1038 to COPANT 331, 1038 to COPANT 333, 1039 to COPANT 333, 1040 to COPANT 330, 1040 to COPANT 331, 1040 to COPANT 333 |
| UK: 080M36 to BS 970/1, 080M40 to BS 970/1, 170H41 to BS 970/1 |
| USA: 1038, 1038 to ASTM A29/A29M, 1038 to ASTM A568/A568M, 1038 to SAE J403, 1039, 1039 to ASTM A29/A29M, 1039 to ASTM A568/A568M, 1039 to SAE J403, 1040, 1040 to ASTM A29/A29M, 1040 to ASTM A513, 1040 to ASTM A519, 1040 to ASTM A568/A568M, 1040 to DoD-F-24669/1, 1040 to FED QQ-S-635B, 1040 to SAE J403, 1042, 1042 to ASTM A29/A29M, 1042 to ASTM A568/A568M, 1042 to SAE J403, 1043, 1043 to ASTM A29/A29M, 1043 to ASTM A568/A568M, 1043 to SAE J403, 1544, C1042 to FED QQ-S-635B, C4 to MIL-S-16788A, CS1040 to MIL-S-11310E, G10380 to ASTM A510/A510M, G10380 to ASTM A576-90b, G10390 to ASTM A510/A510M, G10390 to ASTM A576-90b, G10400 to ASTM A510/A510M, G10400 to ASTM A576-90b, G10420 to ASTM A510/A510M, G10420 to ASTM A576-90b, G10430 to ASTM A510/A510M, G10430 to ASTM A576-90b, UNS G10380, UNS G10380 to UNS, UNS G10390, UNS G10390 to UNS, UNS G10400, UNS G10400 to UNS, UNS G10420, UNS G10420 to UNS, UNS G10430, UNS G10430 to UNS |
| Tradenames: ALLENOY 1038, ASCOMETAL XC38H1-H2, B/43, BOFORS N91, BOHLER V943, DODGE D-4, DONEGAL D-3, DYNAMIC C-1-4, DYNAMIC C-1-5, FORTUNA W3, GREDE 37, HECLA 37, JESSOP A-5, JESSOP STEEL A-5 (S M-40), KRUPP 1730, RED DIAMOND 9S, S/39, SODING WM, SWB-40M4, TULIPE EXTRA NO. 7, UGINE B 38, V4 |