Medium and High Carbon Steel Overview

Medium carbon steels contain about 0.30–0.60% carbon and high carbon steels about 0.60–1.0%. The extra carbon allows the steel to be hardened by quenching and then tempered to the required balance of strength and toughness. Medium carbon grades such as AISI 1040 and 1045 are used for shafts, axles, gears and forgings; high carbon grades such as AISI 1080 and 1095 are used for springs, blades, wire and wear parts.

Oil Quenching vs Water Quenching

Plain carbon steels have low hardenability, so the quench medium matters. Water quenching cools faster and gives higher hardness and strength after tempering, but increases distortion and the risk of quench cracking, especially in higher carbon grades and complex shapes. Oil quenching is gentler and safer for intricate parts, at the cost of lower as-quenched hardness. Where the data sheets include both, the comparison posts show oil and water quenched values tempered at 205, 315, 425, 540 and 650°C side by side.

Tempering Temperature and Properties

After quenching, tempering at a low temperature such as 205°C keeps hardness and tensile strength high, while tempering at 540–650°C lowers strength but greatly improves ductility and toughness. Annealed, as rolled and normalized data sheets are also listed for each grade.

Resulfurized Medium Carbon Steels

AISI 1137, 1141 and 1144 combine medium carbon strength with added sulfur for fast machining, making them popular for shafts, studs and spindles. Compare them with AISI 1117, 1118 and 12L14 in our resulfurized free-machining steels comparison.

Medium and High Carbon Steel Parts from Turkey

Looking for medium or high carbon steel parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1040, 1050, 1095 and 1144 steel parts in-house, heat treated to the condition you specify, and inspects them before shipment. See also low carbon steel grades and low alloy steel grades.

Medium and High Carbon Steel Grades and Data Sheets

Medium carbon steels (1030–1060)

AISI 1030 Medium Carbon Steel

AISI 1040 Medium Carbon Steel

AISI 1050 Medium Carbon Steel

AISI 1060 Medium Carbon Steel

High carbon steels (1080, 1095)

AISI 1080 High Carbon Steel

AISI 1095 High Carbon Steel

Resulfurized medium carbon steels (11xx)

AISI 1137 Resulfurized Medium Carbon Steel

AISI 1141 Resulfurized Medium Carbon Steel

AISI 1144 Resulfurized Medium Carbon Steel

Manganese steel (13xx)

AISI 1340 Medium Carbon Manganese Steel