Aluminum A356.0 permanent mold cast T6 Processing Properties
| Property | Value | Unit |
|---|---|---|
| Metal Casting | Excellent | – |
| Metal Cold Forming | Unsuitable | – |
| Metal Hot Forming | Unsuitable | – |
| Metal Press Forming | Unsuitable | – |
| Metal Deep Drawing | Unsuitable | – |
| Machining Speed | 88.4 | m/min |
| Weldability | Excellent (Note: Preheating is not required, post weld heat treatment is required) | – |
| Aluminum A356.0 permanent mold cast T6 Processing Properties |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey