Aluminum, A356.0, permanent mold cast, T6 | Mechanical Properties

Aluminum A356.0 permanent mold cast T6 Mechanical Properties Property Value Range Unit Young’s Modulus 71.5 – 74.5 GPa Specific Stiffness 26.6 – 27.8 MN·m/kg Yield Strength (Elastic Limit) 241 – 263 MPa Tensile Strength 283 – 307 MPa Specific Strength 89.9 – 98.3 kN·m/kg Elongation 2.5 – 3 % strain Compressive Strength 109 – 121 … Continue reading Aluminum, A356.0, permanent mold cast, T6 | Mechanical Properties