Aluminum A356.0 permanent mold cast T6 Equivalent Grades
| Property | Value |
|---|---|
| Designation | A356.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A13560 |
| EN Number | EN AC-42000 / EN AC-Al Si7Mg |
| Aluminum A356.0 permanent mold cast T6 Equivalent Grades |
Aluminum A356.0 permanent mold cast T6 Standards with Similar Compositions:
| Country | Standard Designations |
|---|---|
| Australia | AA601 to AS 1874, AC601 to AS 1874, CC601 to AS 1874 |
| Austria | AlSi7Mg to ONORM M3429 |
| Belgium | AlSi7Mg to NBN P21-101 |
| Canada | SC70P to CSA, SG70P to CSA HA.3 |
| Czech Republic | 424334 to CSN |
| Europe | EN AB-42100 to CEN EN 1676, EN AC-42100 to CEN EN 1706 |
| Germany | 3.2371/AlSi7Mg to DIN 1725-2 |
| India | 4458 to IS 202 |
| International | AlSi7Mg to ISO 3522 |
| Japan | AC4C.2 to JIS H2211, AC4CH.1 to JIS H2211, AC4CH.2 to JIS H2211 |
| Norway | 17540 to NS 17540 |
| Russia | AL9-1 to GOST 2685 |
| South Africa | 42100 (Al-Si7Mg) to SABS 991, SA14 (Al-Si7MgA) to SABS 989 |
| Switzerland | AlSi7Mg to VSM 10895/21 |
| USA | A13560 to SAE J452, A356.0, A356.0 to ASTM B108, A356.0 to ASTM B618, A356.0 to ASTM B686, A356.1, A356.2, A356.2 to ASTM B179, A356.2 to QQ A-371F, B356.0, C356.0, F356.0, F356.2, UNS A13560, UNS A13561, UNS A13562, UNS A23560, UNS A33560, UNS A43560, UNS A43561, UNS A63560, UNS A63562 |
| Aluminum A356.0 permanent mold cast T6 Standards with Similar Compositions |
Aluminum A356.0 permanent mold cast T6 Tradenames
| Tradename |
|---|
| ALCAN 135 |
| ALCOTEC R-A356.0 |
| ALLCAST 46-10 |
| ALLCAST 46A |
| AP601 |
| BP601 |
| CP 601 |
| DUCTALUMINUM 356S |
| Aluminum A356.0 permanent mold cast T6 Tradenames |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey