Aluminum, A356.0, permanent mold cast, T6 General Information

Aluminum A356.0 permanent mold cast T6 General Information Property Value Designation A356.0 (Aluminum Association) Condition T6 (Solution heat-treated and artificially aged) UNS Number A13560 EN Number EN AC-42000 / EN AC-Al Si7Mg Aluminum A356.0 permanent mold cast T6 General Information Aluminum A356.0 permanent mold cast T6 Typical Uses Industry/Application Specific Use Automotive Industry Space frames … Continue reading Aluminum, A356.0, permanent mold cast, T6 General Information