Aluminum, A356.0, permanent mold cast, T6 | Equivalent Grades
Aluminum A356.0 permanent mold cast T6 Equivalent Grades Property Value Designation A356.0 (Aluminum Association) Condition T6 (Solution heat-treated and artificially aged) UNS Number A13560 EN Number EN AC-42000 / EN AC-Al Si7Mg Aluminum A356.0 permanent mold cast T6 Equivalent Grades Aluminum A356.0 permanent mold cast T6 Standards with Similar Compositions: Country Standard Designations Australia AA601 … Continue reading Aluminum, A356.0, permanent mold cast, T6 | Equivalent Grades