Aluminum A356.0 permanent mold cast T6 General Information
| Property | Value |
|---|---|
| Designation | A356.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A13560 |
| EN Number | EN AC-42000 / EN AC-Al Si7Mg |
| Aluminum A356.0 permanent mold cast T6 General Information |
Aluminum A356.0 permanent mold cast T6 Typical Uses
| Industry/Application | Specific Use |
|---|---|
| Automotive Industry | Space frames |
| Wheels | |
| Axle housings | |
| Differential housings | |
| Pump and Meter Components | Pumps |
| Meters | |
| Engine and Transmission Parts | Intake manifolds |
| Electronics | Electronic cases |
| Fuel Systems | Fuel pumps |
| Aluminum A356.0 permanent mold cast T6 Typical Uses |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey