Aluminum A356.0 permanent mold cast T6 Mechanical Properties
| Property | Value Range | Unit |
|---|---|---|
| Young’s Modulus | 71.5 – 74.5 | GPa |
| Specific Stiffness | 26.6 – 27.8 | MN·m/kg |
| Yield Strength (Elastic Limit) | 241 – 263 | MPa |
| Tensile Strength | 283 – 307 | MPa |
| Specific Strength | 89.9 – 98.3 | kN·m/kg |
| Elongation | 2.5 – 3 | % strain |
| Compressive Strength | 109 – 121 | MPa |
| Flexural Modulus | 71.5 – 74.5 | GPa |
| Flexural Strength (Modulus of Rupture) | 241 – 263 | MPa |
| Shear Modulus | 26.7 – 28.2 | GPa |
| Bulk Modulus | 66.9 – 76.6 | GPa |
| Poisson’s Ratio | 0.322 – 0.338 | – |
| Shape Factor | 27 | – |
| Hardness – Vickers | 100 – 110 | HV |
| Elastic Stored Energy (Springs) | 399 – 475 | kJ/m³ |
| Fatigue Strength at 10⁷ Cycles | 100 – 116 | MPa |
| Fatigue Strength Model (Stress Range) | 96.7 – 120 | MPa |
| Aluminum A356.0 permanent mold cast T6 Mechanical Properties |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey