Aluminum 6005A Equivalent Grades – Similar Compositions

Designation: Aluminum 6005A

6005A, wrought
ConditionsT1, T4, T5, T6
UNS numberA96005A
EN nameEN AW-6005A
EN number3.3210
ISO nameAl SiMg(A)
JIS (Japanese) nameA6NO1

Aluminum 6005A Equivalent Grades – Similar Compositions

Australia: 6005A to AS 2848.1
Austria: AlMgSi0.9 to ONORM M3430
Europe: EN AW-6005A to CEN EN 573-3, EN AW-6081 to CEN EN 573-3
Finland: E-AlMgSi to SFS 2592
India: HG9 to IS 739
International: AlMgSi to ISO/R 827, AlMgSi to ISO/TR 2778, AlSiMg(A) to ISO 209-1
Japan: A6N01S to JIS H4100
Norway: 17303 to NS 17303
USA: 6005A, 6005A to ASTM B221M, 6017, 6081, 6963, UNS A96017, UNS A96081, UNS A96963
Yugoslavia: 3.4551.00/AlSi0.7Mg to JUS C.C2.100

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey