Aluminum 6005A T1 Mechanical Properties

Designation: Aluminum 6005A T1 6005A, wrought Condition T1 (Cooled from elevated temperature shaping process and naturally aged) UNS number A96005A EN name EN AW-6005A EN number 3.3210 ISO name Al SiMg(A) JIS (Japanese) name A6NO1 Mechanical properties: Aluminum 6005A T1 Young’s modulus 67.8 – 71.2 GPa Specific stiffness 25 – 26.3 MN.m/kg Yield strength (elastic … Continue reading Aluminum 6005A T1 Mechanical Properties