Aluminum 6005A Chemical Composition

Designation: Aluminum 6005A

6005A, wrought
ConditionsT1, T4, T5, T6
UNS numberA96005A
EN nameEN AW-6005A
EN number3.3210
ISO nameAl SiMg(A)
JIS (Japanese) nameA6NO1

Composition detail: Aluminum 6005A

Al (aluminum)96.5–99.1%
Cr (chromium)0–0.3%
Cu (copper)0–0.3%
Fe (iron)0–0.35%
Mg (magnesium)0.4–0.7%
Mn (manganese)0–0.5%
Si (silicon)0.5–0.9%
Ti (titanium)0–0.1%
Zn (zinc)0–0.2%
Other0–0.15%

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey