Aluminum 6005A T1 Mechanical Properties

Designation: Aluminum 6005A T1

6005A, wrought
ConditionT1 (Cooled from elevated temperature shaping process and naturally aged)
UNS numberA96005A
EN nameEN AW-6005A
EN number3.3210
ISO nameAl SiMg(A)
JIS (Japanese) nameA6NO1

Mechanical properties: Aluminum 6005A T1

Young’s modulus67.8–71.2GPa
Specific stiffness25–26.3MN.m/kg
Yield strength (elastic limit)100–117MPa
Tensile strength170–198MPa
Specific strength36.9–43.2kN.m/kg
Elongation15–21.6% strain
Compressive strength100–117MPa
Flexural modulus67.8–71.2GPa
Flexural strength (modulus of rupture)100–117MPa
Shear modulus27.1–28.5GPa
Bulk modulus67.8–71.2GPa
Poisson’s ratio0.325–0.335 
Shape factor39.2   
Hardness – Vickers60–63HV
Elastic stored energy (springs)72.3–98.1kJ/m^3
Fatigue strength at 10^7 cycles74.2–86.5MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles67.8–94.7MPa

Impact & fracture properties: Aluminum 6005A T1

Fracture toughness30–36MPa.m^0.5
Toughness (G)13–18.5kJ/m^2

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey