Designation: Aluminum 6005A T5 6005A, wrought Condition T5 (Cooled from an elevated-temperature shaping process and artificially aged) UNS number A96005A EN name EN AW-6005A EN number 3.3210 ISO name Al SiMg(A) JIS (Japanese) name A6NO1 Mechanical properties: Aluminum 6005A T5 Young’s modulus 67.5 – 71 GPa Specific stiffness 24.9 – 26.3 MN.m/kg Yield strength (elastic … Continue reading Aluminum 6005A T5 Mechanical Properties