Designation: Aluminum 6005A 6005A, wrought Conditions T1, T4, T5, T6 UNS number A96005A EN name EN AW-6005A EN number 3.3210 ISO name Al SiMg(A) JIS (Japanese) name A6NO1 Composition detail: Aluminum 6005A Al (aluminum) 96.5 – 99.1 % Cr (chromium) 0 – 0.3 % Cu (copper) 0 – 0.3 % Fe (iron) 0 – 0.35 … Continue reading Aluminum 6005A Chemical Composition